Modifying Digital Occlusal Spacer Effect on the Marginal Gap of Zirconia-Reinforced Lithium Silicate Crowns: In Vitro Scanning Electron Microscopy Evaluation.
A clinically acceptable marginal gap (< 120 µm) was obtained for all three occlusal spacers (60, 90, 120 µm), and as the digital occlusal spacer was reduced the marginal gap reduced as well. The 120-µm occlusal spacer showed a significantly higher marginal gap compared to 90 and 60 µm. The digital occlusal spacer that should be favorable for ZLS crowns is 60 µm.
Authors
- Gil Ben-Izhack (ORCID: https://orcid.org/0000-0001-5482-0264)
- Asaf Shely (ORCID: https://orcid.org/0000-0003-3436-4411)
- Samir E. Bishara
- Omer Koton
- Joseph Nissan (ORCID: https://orcid.org/0000-0001-7290-4357)
- Diva Lugassy (ORCID: https://orcid.org/0000-0002-4614-0493)
- Leon Eliasaf
Publication Details
- Journal
- PubMed
- Published
- 2026-01-22
- DOI
- https://doi.org/10.11607/ijp.9188
- Citations
- 1
- Primary Topic
- Pigment Synthesis and Properties
- Type
- article
- Field-Weighted Citation Impact
- 0.00