CdWO4 Crystal: Thermal Expansion Coefficients, High-Temperature Photoluminescence

High-temperature properties of the CdWO4 cadmium tungstate crystal are studied. This crystal has broad practical applications, e.g. as a scintillator, due to its optical and radiative properties. CdWO4 preserves high structural stability up to 1150 °C and begins to decompose at 1200 °C. Crystal lattice parameters and thermal expansion coefficients are calculated. The latter exhibit the largest expansion along the b axis. High transmittance of the studied sample in the ~0.32-5.0 µm range confirms high optical quality of the crystal and its prospects in photonic applications. The photoluminescence study in the 23-200 °C range reveals two types of luminescence transitions E1 and E2 and shows that the intensity of the spectrum decreases with increasing temperature and vanishes at 200 °C. It is shown that the tendency of intensity decrease depends on the excitation wavelength.

Authors

Institutions

Publication Details

Journal
Journal of Structural Chemistry
Published
2025-04-01
DOI
https://doi.org/10.1134/s0022476625040110
Primary Topic
Luminescence Properties of Advanced Materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

CdWO4 Crystal: Thermal Expansion Coefficients, High-Temperature Photoluminescence

A.E. Musikhin, V. D. Grigorieva, Alexey A. Ryadun, A.B. Kuznetsov et al.
Journal of Structural Chemistry
Luminescence Properties of Advanced Materials
article

CdWO4 Crystal: Thermal Expansion Coefficients, High-Temperature Photoluminescence

A.E. Musikhin, V. D. Grigorieva, Alexey A. Ryadun, A.B. Kuznetsov, A. P. Elisseyev
article en

Abstract

High-temperature properties of the CdWO4 cadmium tungstate crystal are studied. This crystal has broad practical applications, e.g. as a scintillator, due to its optical and radiative properties. CdWO4 preserves high structural stability up to 1150 °C and begins to decompose at 1200 °C. Crystal lattice parameters and thermal expansion coefficients are calculated. The latter exhibit the largest expansion along the b axis. High transmittance of the studied sample in the ~0.32-5.0 µm range confirms high optical quality of the crystal and its prospects in photonic applications. The photoluminescence study in the 23-200 °C range reveals two types of luminescence transitions E1 and E2 and shows that the intensity of the spectrum decreases with increasing temperature and vanishes at 200 °C. It is shown that the tendency of intensity decrease depends on the excitation wavelength.

Journal of Structural ChemistryVol. 66(4)
Novosibirsk State University (RU), V.S. Sobolev Institute of Geology and Mineralogy (RU), Nikolaev Institute of Inorganic Chemistry (RU)
Affordable and clean energy
Openalex Percentile: Top 93%
Luminescence Properties of Advanced Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.