Flotation of a mineralized structure to decrease arsenic content in gold concentrate

Arsenic is a penalty element in flotation concentrates, thus decreasing their quality. Consequently, the present investigation is developed with the objective of carrying out the flotation of a mineralized structure to reduce the content of arsenic “As” in the gold concentrate “Au”. For this purpose, sampling was carried out in a vetiform hydrothermal deposit taking 2 kg for Au-As chemical and mineralogical analysis and two flotation tests in a Rougher stage with the same entry conditions, i.e. Au grade equal to 11.46 g/t and As 1.81%. The results indicate that in test 1 the As content in the concentrate was 4.57%, while in test 2 the As grade in the concentrate was 4.86%, considering that in the latter, in addition to the reagents used in test 1, copper sulfate was applied as an activator, where no sulfide depression was evidenced. Finally, it is concluded that with the experimentation developed, the mineral presented a positive response to the flotation process, achieving the expected result with trial 1, also taking into account the dosage of the reagents used.

Authors

Institutions

Publication Details

Journal
Reincisol
Published
2025-04-22
DOI
https://doi.org/10.59282/reincisol.v4(7)2425-2447
Primary Topic
Metal Extraction and Bioleaching
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Flotation of a mineralized structure to decrease arsenic content in gold concentrate

Carlos Del Valle Jurado, Diego Geovanny Ramos Armijos
Reincisol
Metal Extraction and Bioleaching
article

Flotation of a mineralized structure to decrease arsenic content in gold concentrate

Carlos Del Valle Jurado, Diego Geovanny Ramos Armijos
article en

Abstract

Arsenic is a penalty element in flotation concentrates, thus decreasing their quality. Consequently, the present investigation is developed with the objective of carrying out the flotation of a mineralized structure to reduce the content of arsenic “As” in the gold concentrate “Au”. For this purpose, sampling was carried out in a vetiform hydrothermal deposit taking 2 kg for Au-As chemical and mineralogical analysis and two flotation tests in a Rougher stage with the same entry conditions, i.e. Au grade equal to 11.46 g/t and As 1.81%. The results indicate that in test 1 the As content in the concentrate was 4.57%, while in test 2 the As grade in the concentrate was 4.86%, considering that in the latter, in addition to the reagents used in test 1, copper sulfate was applied as an activator, where no sulfide depression was evidenced. Finally, it is concluded that with the experimentation developed, the mineral presented a positive response to the flotation process, achieving the expected result with trial 1, also taking into account the dosage of the reagents used.

ReincisolVol. 4(7)
National University of San Marcos (PE)
Openalex Percentile: Top 92%
Metal Extraction and Bioleaching
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.