A systematic implementation of the solid electrolyte interphase layer and study of its impact on lithium plating morphology in lithium metal batteries

Dendrite growth and non-uniform deposition at the anode-electrolyte interface pose safety concerns and hinder the commercialization of high energy density , rechargeable lithium metal batteries . Li deposition is influenced by many factors including surface chemistries, such as reaction rate and interfacial energy , local Li + concentration gradients , and surface heterogeneities . In particular, the Solid Electrolyte Interphase (SEI) layer is a key factor causing instability at the interface. However, the embedded nature of the anode-electrolyte interface makes it difficult to observe and study experimentally; alternatively, computational modeling can explicitly resolve the interface and be an effective tool to understand Li deposition behavior . The SEI layer is a chemically complex, dynamic layer that is not well understood. In this paper a novel computational model is used to evaluate three computational approaches to implement the SEI, which allows for a manageable, yet representative incorporation of this layer. These approaches are then combined to study how the physical parameters of the SEI layer impact plating stability showing that thin and highly conductive layers with large interfacial energies can aid in suppressing dendrite growth. Finally, the complexity that is required to accurately capture the SEI physics is evaluated and presented indicating that it is critical to consider the impact that the SEI layer has on the Li ion transport and interfacial energy . Additionally, for complex interfacial geometries, like mechanically patterned anodes, a non-uniform reaction rate and breaks in the SEI layer are important to consider. • Computational model developed to simulate electrodeposition in lithium batteries. • Captures the impact of the solid electrolyte interphase (SEI) layer. • Impact of the SEI layer can be captured using simplified methods. • LiF-rich SEI layer results in stable lithium plating morphologies. • Thin and highly conductive SEI layers lead to uniform Li deposition.

Authors

Institutions

Publication Details

Journal
Journal of Energy Storage
Published
2025-04-22
DOI
https://doi.org/10.1016/j.est.2025.116731
Citations
3
Primary Topic
Advancements in Battery Materials
Type
article
Field-Weighted Citation Impact
2.19

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

A systematic implementation of the solid electrolyte interphase layer and study of its impact on lithium plating morphology in lithium metal batteries

Madison Morey, Emily Ryan, Maya Lobel
3 citations
Journal of Energy Storage
Advancements in Battery Materials
2.19
article

A systematic implementation of the solid electrolyte interphase layer and study of its impact on lithium plating morphology in lithium metal batteries

Madison Morey, Emily Ryan, Maya Lobel
article en
3 citations

Abstract

Dendrite growth and non-uniform deposition at the anode-electrolyte interface pose safety concerns and hinder the commercialization of high energy density , rechargeable lithium metal batteries . Li deposition is influenced by many factors including surface chemistries, such as reaction rate and interfacial energy , local Li + concentration gradients , and surface heterogeneities . In particular, the Solid Electrolyte Interphase (SEI) layer is a key factor causing instability at the interface. However, the embedded nature of the anode-electrolyte interface makes it difficult to observe and study experimentally; alternatively, computational modeling can explicitly resolve the interface and be an effective tool to understand Li deposition behavior . The SEI layer is a chemically complex, dynamic layer that is not well understood. In this paper a novel computational model is used to evaluate three computational approaches to implement the SEI, which allows for a manageable, yet representative incorporation of this layer. These approaches are then combined to study how the physical parameters of the SEI layer impact plating stability showing that thin and highly conductive layers with large interfacial energies can aid in suppressing dendrite growth. Finally, the complexity that is required to accurately capture the SEI physics is evaluated and presented indicating that it is critical to consider the impact that the SEI layer has on the Li ion transport and interfacial energy . Additionally, for complex interfacial geometries, like mechanically patterned anodes, a non-uniform reaction rate and breaks in the SEI layer are important to consider. • Computational model developed to simulate electrodeposition in lithium batteries. • Captures the impact of the solid electrolyte interphase (SEI) layer. • Impact of the SEI layer can be captured using simplified methods. • LiF-rich SEI layer results in stable lithium plating morphologies. • Thin and highly conductive SEI layers lead to uniform Li deposition.

Journal of Energy StorageVol. 122
Boston University (US)
National Science Foundation, Boston University
Openalex Percentile: Top 13%
Advancements in Battery Materials
2.19
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.