Na layer pillar ion post-doping facilitates diffusion kinetics and structural stability in NaNi<sub>0.5</sub>Mn<sub>0.5</sub>O<sub>2</sub>

Compared to Ca pre-doping inhibiting pure-phase formation, the Ca post-doping strategy enables the synthesis of structurally stable NaNi 0.5 Mn 0.5 O 2 cathodes with fast Na + diffusion kinetics.

Authors

Institutions

Publication Details

Journal
Journal of Materials Chemistry A
Published
2025-01-01
DOI
https://doi.org/10.1039/d5ta00764j
Citations
2
Primary Topic
Ferroelectric and Piezoelectric Materials
Type
article
Field-Weighted Citation Impact
1.04
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Na layer pillar ion post-doping facilitates diffusion kinetics and structural stability in NaNi0.5Mn0.5O2

Zhian Zhang, Ziyue Qiu, Shihao Li, Yanqing Lai et al.
2 citations
Journal of Materials Chemistry A
Ferroelectric and Piezoelectric Materials
1.04
article

Na layer pillar ion post-doping facilitates diffusion kinetics and structural stability in NaNi0.5Mn0.5O2

Zhian Zhang, Ziyue Qiu, Shihao Li, Yanqing Lai, Wei Dong Zhou, Yuhang Zhang, Yi Zhang, Jie Li, Rui Jin, Huiru Wang
article en
2 citations

Abstract

Compared to Ca pre-doping inhibiting pure-phase formation, the Ca post-doping strategy enables the synthesis of structurally stable NaNi 0.5 Mn 0.5 O 2 cathodes with fast Na + diffusion kinetics.

Journal of Materials Chemistry AVol. 13(19)
Central South University (CN)
Openalex Percentile: Top 27%
Ferroelectric and Piezoelectric Materials
1.04
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.