Investigation of Compression, Flexural, Impact, Hardness, Density Characteristics of Composites Reinforced with Coir, Corn Fibers

This work investigated the combination of 20 wt.% of natural fibers (coconut coir fiber and corn silk) with 80 wt.% of unsaturated polyester resin. The coir and corn fibers were washed and dehydrated by sunlight and then treated with an alkali solution after that, they dried for 20 minutes at 60°C in the furnace to reduce the moisture content. Grinding and sieving processes are carried out to attend to a particle size of 0.9 mm. The natural fiber-reinforced polymer (NFRP) composites were manufactured at room temperature through an open glass mold. The mechanical properties of coconut coir fiber reinforced polymer (CCFRP) and corn silk fiber reinforced polymer (CSFRP) composites are evaluated using compression, flexural, impact, and hardness according to ASTM standards D695, D790, D256, and D2240, CCFRP composite shows higher properties than CSFRP composite with 25%, 24.324%, 20%, 3.703% respectively. The CSFRP composite shows a higher density than the CCFRP composite with a percentage of 2.895%.

Authors

Publication Details

Journal
Panamerican mathematical journal.
Published
2025-03-25
DOI
https://doi.org/10.52783/pmj.v35.i4s.4464
Citations
1
Primary Topic
Natural Fiber Reinforced Composites
Type
article
Field-Weighted Citation Impact
0.61
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Investigation of Compression, Flexural, Impact, Hardness, Density Characteristics of Composites Reinforced with Coir, Corn Fibers

Sanad Abdulkareem Ismael
1 citations
Panamerican mathematical journal.
Natural Fiber Reinforced Composites
0.61
article

Investigation of Compression, Flexural, Impact, Hardness, Density Characteristics of Composites Reinforced with Coir, Corn Fibers

Sanad Abdulkareem Ismael
article en
1 citations

Abstract

This work investigated the combination of 20 wt.% of natural fibers (coconut coir fiber and corn silk) with 80 wt.% of unsaturated polyester resin. The coir and corn fibers were washed and dehydrated by sunlight and then treated with an alkali solution after that, they dried for 20 minutes at 60°C in the furnace to reduce the moisture content. Grinding and sieving processes are carried out to attend to a particle size of 0.9 mm. The natural fiber-reinforced polymer (NFRP) composites were manufactured at room temperature through an open glass mold. The mechanical properties of coconut coir fiber reinforced polymer (CCFRP) and corn silk fiber reinforced polymer (CSFRP) composites are evaluated using compression, flexural, impact, and hardness according to ASTM standards D695, D790, D256, and D2240, CCFRP composite shows higher properties than CSFRP composite with 25%, 24.324%, 20%, 3.703% respectively. The CSFRP composite shows a higher density than the CCFRP composite with a percentage of 2.895%.

Panamerican mathematical journal.Vol. 35(4s)
Openalex Percentile: Top 38%
Natural Fiber Reinforced Composites
0.61
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.