Optimising the Selective Leaching and Recovery of Cobalt, Lanthanum, and Strontium for Recycling End-of-Life Solid Oxide Cells
This study explored the selective recovery of Co, La, and Sr from end-of-life solid oxide cells (SOCs) using ultrasound-assisted leaching in HCl. HCl concentration (1, 5, and 10 M) and solid-to-liquid ratio (S/L, 100 and 200 g/L) were varied to optimize the efficiency and the selectivity of Co, La, and Sr leaching. Then, they were recovered as oxalates at pH 0.7, 1, and 4. Using 10 M HCl and an S/L ratio of 100 g/L on ball-milled samples achieved 96–99% leaching efficiency but led to Ni impurities from the underneath layers. Thermal pre-treatment at 800 °C decreased Ni leaching by 90% but decreased target metals’ recovery by 9%. Direct leaching (without pre-treatments) with 1 M HCl and an S/L ratio of 200 g/L achieved up to 91% leaching efficiency, recovering 42% of Co, 93% of La, and 33% of Sr with minimal Ni impurities. A preliminary economic analysis indicated that avoiding pre-treatments can cut expenses by 96%. An economic analysis indicated that direct leaching is the most cost effective, reducing expenses by up to 96% compared to thermal pre-treatment and high HCl concentrations. This study highlights the potential for an efficient and cost-effective method for recycling Co, La, and Sr from EoL SOCs.
Authors
- Federico Smeacetto (ORCID: https://orcid.org/0000-0003-0764-5269)
- Martina Bruno (ORCID: https://orcid.org/0000-0002-5674-993X)
- Silvia Fiore (ORCID: https://orcid.org/0000-0001-5949-0559)
- Sonia Fiorilli (ORCID: https://orcid.org/0000-0002-2986-0528)
- Sofia Saffirio (ORCID: https://orcid.org/0009-0009-6691-8360)
Institutions
- Politecnico di Torino (IT)
Publication Details
- Journal
- Batteries
- Published
- 2025-03-25
- DOI
- https://doi.org/10.3390/batteries11040124
- Citations
- 2
- Primary Topic
- Extraction and Separation Processes
- Type
- article
- Field-Weighted Citation Impact
- 1.43