Preparation of Antifouling Composite Coating for Rubber. Part 1: Manufacturing and Laboratory Testing

This article introduces results of investigations on Cu2O concentration on release rate of antifouling composite coating for rubber, effects of fineness on ability to release Cu2O of paint (fineness of paint increases, Cu2O release speed of composite coating decreases), effects of period from composite coating preparation to start testing on ability of Cu2O release. Besides, effects of anti-UV additive on ability of composite coating to withstand from UV-thermo-humidity complex was also investigated. Results show that Cu2O concentration is 25 weight percent (wt. %), fineness of paint is 75-80 µm are suitable, period from composite coating preparation to time for being used is about 5 days for the best antifouling grade while ensuring mechanical properties of composite coating. Anti-UV additive of 1 wt. % is suitable for antifouling composite coating for rubber.

Authors

Institutions

Publication Details

Journal
Malaysian Journal on Composites Science and Manufacturing
Published
2025-03-20
DOI
https://doi.org/10.37934/mjcsm.16.1.3545
Citations
1
Primary Topic
Tribology and Wear Analysis
Type
article
Field-Weighted Citation Impact
0.86
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Preparation of Antifouling Composite Coating for Rubber. Part 1: Manufacturing and Laboratory Testing

Nguyen Ba Ngoc, Thanh Nguyen Trung, Le Thanh Viet, Hoang Ngoc Phuoc et al.
1 citations
Malaysian Journal on Composites Science and Manufacturing
Tribology and Wear Analysis
0.86
article

Preparation of Antifouling Composite Coating for Rubber. Part 1: Manufacturing and Laboratory Testing

Nguyen Ba Ngoc, Thanh Nguyen Trung, Le Thanh Viet, Hoang Ngoc Phuoc, Tran Van Quyen, Truong Dinh Tuan, Ning Hao, Nguyễn Đức Thành
article en
1 citations

Abstract

This article introduces results of investigations on Cu2O concentration on release rate of antifouling composite coating for rubber, effects of fineness on ability to release Cu2O of paint (fineness of paint increases, Cu2O release speed of composite coating decreases), effects of period from composite coating preparation to start testing on ability of Cu2O release. Besides, effects of anti-UV additive on ability of composite coating to withstand from UV-thermo-humidity complex was also investigated. Results show that Cu2O concentration is 25 weight percent (wt. %), fineness of paint is 75-80 µm are suitable, period from composite coating preparation to time for being used is about 5 days for the best antifouling grade while ensuring mechanical properties of composite coating. Anti-UV additive of 1 wt. % is suitable for antifouling composite coating for rubber.

Malaysian Journal on Composites Science and ManufacturingVol. 16(1)
Hanoi University of Industry (VN)
Openalex Percentile: Top 33%
Tribology and Wear Analysis
0.86
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Preparation of Antifouling Composite Coating for Rubber. Part 1: Manufacturing and Laboratory Testing — Nguyen Ba Ngoc, Thanh Nguyen Trung, et al. · Malaysian Journal on Composites Science and Manufacturing (2025) | TGRS Research Map | TGRS