Low threshold polymeric integrated optofluidic microlaser

A low threshold optofluidic microlaser have been achieved using only polymeric materials and lamination process. The resonator is fabricated by two commercially available (3M) plane parallel Bragg mirrors composed of hundred layers with alternating high- and low-index layers of polyester and acrylic polymer with a high reflectivity (R>96%). The cavity, the mirrors and the substrates are assembled by a cold lamination process. This approach simplifies the fabrication procedure while retaining high optical surface quality, resulting in a compact, low-cost disposable device. As gain medium a water solution of Rhodamine B with a concentration of 0.9mM has been employed. A pulsed laser (557 nm wavelength, 5 ns pulse width, 10 Hz repetition rate) normally incident into the FP microcavity through a lens with a focal spot size of 140 μm has been used for the measurements. The device shows a threshold of 1μJ/mm<sup>2</sup> with emission peaks centered at around λ =632 nm.

Authors

Institutions

Publication Details

Published
2025-03-19
DOI
https://doi.org/10.1117/12.3044212
Primary Topic
Photonic and Optical Devices
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Low threshold polymeric integrated optofluidic microlaser

Genni Testa, Romeo Bernini, Gianluca Persichetti
2 links
Photonic and Optical Devices
article

Low threshold polymeric integrated optofluidic microlaser

Genni Testa, Romeo Bernini, Gianluca Persichetti
article en

Abstract

A low threshold optofluidic microlaser have been achieved using only polymeric materials and lamination process. The resonator is fabricated by two commercially available (3M) plane parallel Bragg mirrors composed of hundred layers with alternating high- and low-index layers of polyester and acrylic polymer with a high reflectivity (R>96%). The cavity, the mirrors and the substrates are assembled by a cold lamination process. This approach simplifies the fabrication procedure while retaining high optical surface quality, resulting in a compact, low-cost disposable device. As gain medium a water solution of Rhodamine B with a concentration of 0.9mM has been employed. A pulsed laser (557 nm wavelength, 5 ns pulse width, 10 Hz repetition rate) normally incident into the FP microcavity through a lens with a focal spot size of 140 μm has been used for the measurements. The device shows a threshold of 1μJ/mm<sup>2</sup> with emission peaks centered at around λ =632 nm.

Istituto per il Rilevamento Elettromagnetico dell'Ambiente (IT)
Affordable and clean energy
Openalex Percentile: Top 96%
Photonic and Optical Devices
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.