Effect of Mechanical Activation on the Thermal Oxidation of Sphalerite

We consider the effect of mechanical activation on the particle size and strain of natural sphalerite particles and demonstrate that mechanical activation of the mineral for 20 min in a high-energy planetary mill reduces the crystallite size to 20 nm and that in this process the lattice strain in sphalerite reaches 0.73–0.85%. Thermogravimetry, calorimetry, and mass spectrometry have been used to study sphalerite oxidation processes during nonisothermal heating to a temperature of 1000°C in flowing air before and after mechanical activation. Mechanical activation of sphalerite has been shown to lead to a slight increase in the rate of sulfate formation, a decrease in the temperature and enthalpy of the thermal effects involved, and release of sulfur dioxide as a product of interaction with oxygen starting at a temperature of 150°C.

Authors

Institutions

Publication Details

Journal
Inorganic Materials
Published
2024-11-01
DOI
https://doi.org/10.1134/s0020168525700037
Primary Topic
Minerals Flotation and Separation Techniques
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of Mechanical Activation on the Thermal Oxidation of Sphalerite

С. Х. Эстемирова, R. I. Gulyaeva, К. В. Пикулин, С. В. Сергеева
Inorganic Materials
Minerals Flotation and Separation Techniques
article

Effect of Mechanical Activation on the Thermal Oxidation of Sphalerite

С. Х. Эстемирова, R. I. Gulyaeva, К. В. Пикулин, С. В. Сергеева
article en

Abstract

We consider the effect of mechanical activation on the particle size and strain of natural sphalerite particles and demonstrate that mechanical activation of the mineral for 20 min in a high-energy planetary mill reduces the crystallite size to 20 nm and that in this process the lattice strain in sphalerite reaches 0.73–0.85%. Thermogravimetry, calorimetry, and mass spectrometry have been used to study sphalerite oxidation processes during nonisothermal heating to a temperature of 1000°C in flowing air before and after mechanical activation. Mechanical activation of sphalerite has been shown to lead to a slight increase in the rate of sulfate formation, a decrease in the temperature and enthalpy of the thermal effects involved, and release of sulfur dioxide as a product of interaction with oxygen starting at a temperature of 150°C.

Inorganic MaterialsVol. 60(11)
Russian Academy of Sciences (RU), Institute of Metallurgy (RU)
Clean water and sanitation
Openalex Percentile: Top 73%
Minerals Flotation and Separation Techniques
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Effect of Mechanical Activation on the Thermal Oxidation of Sphalerite — С. Х. Эстемирова, R. I. Gulyaeva, et al. · Inorganic Materials (2024) | TGRS Research Map | TGRS