Local structure of zinc–indium–tin oxide films via grazing-incidence x-ray pair-distribution functions and theoretical methods

A detailed experimental and theoretical study on the local (r ≤ 4.5 Å) atomic structure of amorphous and crystalline zinc–indium–tin oxide (ZITO) thin films using grazing-incidence x-ray Pair-Distribution Functions (PDFs), ab initio Molecular Dynamics (MD), and Empirical Potential Structure Refinement (EPSR) Monte Carlo simulations is presented. High-energy synchrotron x rays, a two-dimensional detector, and different incident angles were used to probe the depth uniformity of five (ZnO)0.15 (In2O3)0.70 (SnO2)0.15 films that were deposited via pulsed-laser deposition at growth temperatures (TG) ranging from 25 to 300 °C. Films deposited at TG ≤ 150 °C were amorphous. The partially crystalline (TG = 200 °C) and fully crystalline (TG = 300 °C) films were highly textured. Both crystalline and amorphous structures were investigated using ab initio MD and EPSR Monte Carlo simulations. The density of the amorphous films determined from the experimental data agreed with MD calculations. Coordination numbers, bond lengths, and distortion for metal–oxygen and for both the edge- and corner-shared In–metal shells up to 4.5 Å obtained from PDF analysis closely agreed with MD and EPSR simulations. There is a pronounced decrease in the edge- and corner-shared In–Zn distances arising from the shorter Zn–O bond length, Zn–O tetrahedral coordination, and In–O–Zn angle in amorphous ZITO compared to its crystalline counterpart. A maximum in electrical mobility was observed for the amorphous film just before crystallization occurred. While the peak is broad, consistent with nearly unchanged overall cation–oxygen coordination in the amorphous films, ESPR results indicate that the tetrahedral coordination follows the conductivity trend.

Authors

Institutions

Publication Details

Journal
Journal of Applied Physics
Published
2025-03-17
DOI
https://doi.org/10.1063/5.0246132
Citations
2
Primary Topic
ZnO doping and properties
Type
article
Field-Weighted Citation Impact
1.04

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Local structure of zinc–indium–tin oxide films via grazing-incidence x-ray pair-distribution functions and theoretical methods

Kaj Edlund, И. А. Журавлев, Omar Medina, Bishal Bhattarai et al.
2 citations
Journal of Applied Physics
ZnO doping and properties
1.04
article

Local structure of zinc–indium–tin oxide films via grazing-incidence x-ray pair-distribution functions and theoretical methods

Kaj Edlund, И. А. Журавлев, Omar Medina, Bishal Bhattarai, John Okasinski, Julia E. Medvedeva, Miko M. Stulajter, Chris J. Benmore, Thomas Holmes, Gabriela B. González, Thomas Bsaibes, Manuel Osorio, R. P. H. Chang, D. Bruce Buchholz, G. Cárdenas, S. Cone, C. Riegger
article en
2 citations

Abstract

A detailed experimental and theoretical study on the local (r ≤ 4.5 Å) atomic structure of amorphous and crystalline zinc–indium–tin oxide (ZITO) thin films using grazing-incidence x-ray Pair-Distribution Functions (PDFs), ab initio Molecular Dynamics (MD), and Empirical Potential Structure Refinement (EPSR) Monte Carlo simulations is presented. High-energy synchrotron x rays, a two-dimensional detector, and different incident angles were used to probe the depth uniformity of five (ZnO)0.15 (In2O3)0.70 (SnO2)0.15 films that were deposited via pulsed-laser deposition at growth temperatures (TG) ranging from 25 to 300 °C. Films deposited at TG ≤ 150 °C were amorphous. The partially crystalline (TG = 200 °C) and fully crystalline (TG = 300 °C) films were highly textured. Both crystalline and amorphous structures were investigated using ab initio MD and EPSR Monte Carlo simulations. The density of the amorphous films determined from the experimental data agreed with MD calculations. Coordination numbers, bond lengths, and distortion for metal–oxygen and for both the edge- and corner-shared In–metal shells up to 4.5 Å obtained from PDF analysis closely agreed with MD and EPSR simulations. There is a pronounced decrease in the edge- and corner-shared In–Zn distances arising from the shorter Zn–O bond length, Zn–O tetrahedral coordination, and In–O–Zn angle in amorphous ZITO compared to its crystalline counterpart. A maximum in electrical mobility was observed for the amorphous film just before crystallization occurred. While the peak is broad, consistent with nearly unchanged overall cation–oxygen coordination in the amorphous films, ESPR results indicate that the tetrahedral coordination follows the conductivity trend.

Journal of Applied PhysicsVol. 137(11)
Northwestern University (US), DePaul University (US), Argonne National Laboratory (US), Missouri University of Science and Technology (US)
National Science Foundation, DePaul University, Office of Science, Materials Research Science and Engineering Center, Northwestern University
Openalex Percentile: Top 27%
ZnO doping and properties
1.04
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.