THE EFFECT OF PROCESS TEMPERATURE CONDITIONS ON THE CHARACTERISTICS OF COMPOSITE PHOTOPOLYMER MATERIAL FOR LASER STEREOLITHOGRAPHY TECHNOLOGY

The article considers the results of a study of a composite material based on Clear Resin V4 photopolymer resin (Formlabs) and crushed cured waste with a particle size of 40–50 microns and a content of 10 wt. %. The influence of printing temperature (23 and 32 °C) and the time of additional treatment with ultraviolet (UV) radiation at a temperature of 60 °C on elastic strength characteristics and the structure of the final product. Increasing the printing temperature and UV treatment improves the elastic-strength properties, while an exposure time of more than 75 minutes is not advisable. Microscopic methods have been used to identify defects that occur when printing parameters are changed. Recommendations on the temperature conditions of the technological process are given.

Authors

Institutions

Publication Details

Journal
Transaction Kola Science Centre
Published
2024-11-28
DOI
https://doi.org/10.37614/2949-1215.2024.15.1.070
Primary Topic
Additive Manufacturing and 3D Printing Technologies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

THE EFFECT OF PROCESS TEMPERATURE CONDITIONS ON THE CHARACTERISTICS OF COMPOSITE PHOTOPOLYMER MATERIAL FOR LASER STEREOLITHOGRAPHY TECHNOLOGY

Galina Stanislavovna Dyakova, Е. И. Кордикова, Viktoryia Khodzer
2 links
Transaction Kola Science Centre
Additive Manufacturing and 3D Printing Technologies
article

THE EFFECT OF PROCESS TEMPERATURE CONDITIONS ON THE CHARACTERISTICS OF COMPOSITE PHOTOPOLYMER MATERIAL FOR LASER STEREOLITHOGRAPHY TECHNOLOGY

Galina Stanislavovna Dyakova, Е. И. Кордикова, Viktoryia Khodzer
article en

Abstract

The article considers the results of a study of a composite material based on Clear Resin V4 photopolymer resin (Formlabs) and crushed cured waste with a particle size of 40–50 microns and a content of 10 wt. %. The influence of printing temperature (23 and 32 °C) and the time of additional treatment with ultraviolet (UV) radiation at a temperature of 60 °C on elastic strength characteristics and the structure of the final product. Increasing the printing temperature and UV treatment improves the elastic-strength properties, while an exposure time of more than 75 minutes is not advisable. Microscopic methods have been used to identify defects that occur when printing parameters are changed. Recommendations on the temperature conditions of the technological process are given.

Transaction Kola Science CentreVol. 15(1)
Belarusian State Technological University (BY)
Openalex Percentile: Top 70%
Additive Manufacturing and 3D Printing Technologies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.