Characteristics of PVD SiCN for Application in Hybrid Cu Bonding

To enhance the density and performance of semiconductor devices, 3D packaging with hybrid Cu bonding is emerging as a critical technology. One of the dielectrics used in hybrid Cu bonding is SiCN, typically deposited using PECVD (plasma-enhanced chemical vapor deposition). In this study, we investigated SiCN deposited at room temperature using PVD (physical vapor deposition). The SiCN, with a thickness of 150 nm, exhibited a surface roughness of 0.3-0.4 nm after the CMP (chemical mechanical polishing) process and a contact angle of about 10 degrees and dielectric constant of 3.9, indicating its potential as a dielectric for hybrid Cu bonding. And, PVD SiCN-SiCN bonding was performed at 260℃, resulting in a uniform and void-free interface.

Authors

Publication Details

Journal
JSTS Journal of Semiconductor Technology and Science
Published
2025-02-28
DOI
https://doi.org/10.5573/jsts.2025.25.1.102
Citations
4
Primary Topic
3D IC and TSV technologies
Type
article
Field-Weighted Citation Impact
2.92
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Characteristics of PVD SiCN for Application in Hybrid Cu Bonding

Junyoung Choi, Suin Jang, Dongmyeong Lee, Sukkyung Kang et al.
4 citations
JSTS Journal of Semiconductor Technology and Science
3D IC and TSV technologies
2.92
article

Characteristics of PVD SiCN for Application in Hybrid Cu Bonding

Junyoung Choi, Suin Jang, Dongmyeong Lee, Sukkyung Kang, Sanha Kim, Eunkyung Kim
article en
4 citations

Abstract

To enhance the density and performance of semiconductor devices, 3D packaging with hybrid Cu bonding is emerging as a critical technology. One of the dielectrics used in hybrid Cu bonding is SiCN, typically deposited using PECVD (plasma-enhanced chemical vapor deposition). In this study, we investigated SiCN deposited at room temperature using PVD (physical vapor deposition). The SiCN, with a thickness of 150 nm, exhibited a surface roughness of 0.3-0.4 nm after the CMP (chemical mechanical polishing) process and a contact angle of about 10 degrees and dielectric constant of 3.9, indicating its potential as a dielectric for hybrid Cu bonding. And, PVD SiCN-SiCN bonding was performed at 260℃, resulting in a uniform and void-free interface.

JSTS Journal of Semiconductor Technology and ScienceVol. 25(1)
Openalex Percentile: Top 10%
3D IC and TSV technologies
2.92
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Characteristics of PVD SiCN for Application in Hybrid Cu Bonding — Junyoung Choi, Suin Jang, et al. · JSTS Journal of Semiconductor Technology and Science (2025) | TGRS Research Map | TGRS