Reinforcing folding boxboard ply stock with refined pulp and its effect on dewatering potential

The folding boxboard (FBB) filler ply typically contains a significant amount of mechanical pulp such as bleached thermomechanical pulp (BTMP), bleached chemi-thermomechanical pulp (BCTMP), and chemi-thermomechanical pulp (CTMP), etc. It is usually reinforced with either refined broke from the same paper machine line and converting process or by utilizing traditional bleached kraft pulp (BKP). In response to the drive for improved/increased ply bond (to avoid undesired delamination), increased bulk, reduced basis weight, and minimized energy consumption, papermakers have experimented with various options and strategies. In between the common approaches, choices have been made between reducing the refining of the mechanical pulp, increasing the broke refining (more frequently practiced on the production scale), or increasing the BKP refining (a potentially superior choice). This study focused on a simplified approach to assess the impact of three reinforcement pulps with different refining levels on the dewatering of the filler ply. The reinforcement pulp was added to the core stock for the FBB filler ply — a mechanical pulp, BCTMP, with a drainability of 25 °SR. The proportions of the reinforcement pulp, hardwood bleached kraft pulp (HWBKP), were 20% of 30-35 °SR, 10% of HWBKP 50-55 °SR, and 5% of HWBKP 70-75 °SR. The intention behind using varying percentages of reinforcement pulp was to attain a controlled internal bond while enhancing bulk through increased mechanical pulp content. The dewatering potential of the stock mixtures was assessed at three vacuum levels — 4, 10, and 25 kPa — that can be found in progressive stages within production- scale forming sections. Our goal was to find an optimal reinforcement strategy for filler ply that would minimize the use of the reinforcement pulp, give better strength, retain bulk, and lower basis weight. The success of this strategy was verified with an actual FBB machine.

Authors

Publication Details

Journal
TAPPI Journal
Published
2025-02-27
DOI
https://doi.org/10.32964/tj24.2.111
Primary Topic
Advanced Cellulose Research Studies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Reinforcing folding boxboard ply stock with refined pulp and its effect on dewatering potential

Antti Koponen, Ari Jäsberg, Juan Cecchini, Merja Selenius
TAPPI Journal
Advanced Cellulose Research Studies
article

Reinforcing folding boxboard ply stock with refined pulp and its effect on dewatering potential

Antti Koponen, Ari Jäsberg, Juan Cecchini, Merja Selenius
article en

Abstract

The folding boxboard (FBB) filler ply typically contains a significant amount of mechanical pulp such as bleached thermomechanical pulp (BTMP), bleached chemi-thermomechanical pulp (BCTMP), and chemi-thermomechanical pulp (CTMP), etc. It is usually reinforced with either refined broke from the same paper machine line and converting process or by utilizing traditional bleached kraft pulp (BKP). In response to the drive for improved/increased ply bond (to avoid undesired delamination), increased bulk, reduced basis weight, and minimized energy consumption, papermakers have experimented with various options and strategies. In between the common approaches, choices have been made between reducing the refining of the mechanical pulp, increasing the broke refining (more frequently practiced on the production scale), or increasing the BKP refining (a potentially superior choice). This study focused on a simplified approach to assess the impact of three reinforcement pulps with different refining levels on the dewatering of the filler ply. The reinforcement pulp was added to the core stock for the FBB filler ply — a mechanical pulp, BCTMP, with a drainability of 25 °SR. The proportions of the reinforcement pulp, hardwood bleached kraft pulp (HWBKP), were 20% of 30-35 °SR, 10% of HWBKP 50-55 °SR, and 5% of HWBKP 70-75 °SR. The intention behind using varying percentages of reinforcement pulp was to attain a controlled internal bond while enhancing bulk through increased mechanical pulp content. The dewatering potential of the stock mixtures was assessed at three vacuum levels — 4, 10, and 25 kPa — that can be found in progressive stages within production- scale forming sections. Our goal was to find an optimal reinforcement strategy for filler ply that would minimize the use of the reinforcement pulp, give better strength, retain bulk, and lower basis weight. The success of this strategy was verified with an actual FBB machine.

TAPPI JournalVol. 24(2)
Openalex Percentile: Top 98%
Advanced Cellulose Research Studies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.