Dentin cavity pretreatments to improve the bond strength of direct and CAD/CAM restorations using resin composite

Dentin cavity wall pretreatments to improve the bond strength of direct and computer-aided design/computer-aided manufacturing (CAD/CAM) restorations using resin composite were examined. Experiment 1 divided 18 standardized MOD cavities into three conditions: no pretreatment (Group N, control); chemical pretreatment with EDTA solution (Group C); and mechanical pretreatment with glycine air-powder polishing (Group M). Specimens were restored using direct resin composites. Micro-tensile bond strength (μ-TBS) was measured after cyclic loading. The μ-TBS was significantly higher for Groups C and M than for Group N. Group M showed the best bonding reliability. In Experiment 2, cavity preparation, dentin pretreatment, cyclic loading, and μ-TBS testing were performed using the same methods applied in Experiment 1. Specimens were restored using CAD/CAM resin composite inlays. The μ-TBS was significantly higher for Groups C and M than for Group N. No significant difference in bonding reliability was apparent among all groups.

Authors

Institutions

Publication Details

Journal
Dental Materials Journal
Published
2025-03-04
DOI
https://doi.org/10.4012/dmj.2024-220
Primary Topic
Dental materials and restorations
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Dentin cavity pretreatments to improve the bond strength of direct and CAD/CAM restorations using resin composite

Toshio Maseki, Ruth H. Sugiyama
Dental Materials Journal
Dental materials and restorations
article

Dentin cavity pretreatments to improve the bond strength of direct and CAD/CAM restorations using resin composite

Toshio Maseki, Ruth H. Sugiyama
article en

Abstract

Dentin cavity wall pretreatments to improve the bond strength of direct and computer-aided design/computer-aided manufacturing (CAD/CAM) restorations using resin composite were examined. Experiment 1 divided 18 standardized MOD cavities into three conditions: no pretreatment (Group N, control); chemical pretreatment with EDTA solution (Group C); and mechanical pretreatment with glycine air-powder polishing (Group M). Specimens were restored using direct resin composites. Micro-tensile bond strength (μ-TBS) was measured after cyclic loading. The μ-TBS was significantly higher for Groups C and M than for Group N. Group M showed the best bonding reliability. In Experiment 2, cavity preparation, dentin pretreatment, cyclic loading, and μ-TBS testing were performed using the same methods applied in Experiment 1. Specimens were restored using CAD/CAM resin composite inlays. The μ-TBS was significantly higher for Groups C and M than for Group N. No significant difference in bonding reliability was apparent among all groups.

Dental Materials JournalVol. 44(2)
Nippon Dental University (JP)
Openalex Percentile: Top 96%
Dental materials and restorations
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics