The critical role of the anode porous transport layer/catalyst layer interface of polymer electrolyte membrane water electrolyzers: A parametric analysis

Reducing the dependency of proton exchange membrane water electrolyzers (PEMWE) on precious metals, such as iridium (Ir), is necessary to develop a widespread green hydrogen system. This challenge requires a careful design of the interface between the anode porous transport layer (PTL) and the catalyst layer (CL). A comprehensive numerical analysis of relevant parameters that govern the behavior of the anode PTL/CL interface is presented. Calculations are also combined with an experimental characterization of the thickness and electrical conductivity of an unsupported CL as a function of Ir loading. The results show that the in-plane electrical resistance at the anode PTL/CL interface plays a critical role in cell performance. Reaching an acceptable electrical resistance at low Ir loading ( L Ir ≃ 0 . 1 mg Ir , cm − 2 ) can be accomplished through the incorporation of a micrometer-sized microporous layer (MPL) onto the PTL or the preparation of bimodal CLs with a secondary conductive phase. Further reduction of the Ir loading to the ultra-low regime ( L Ir ≲ 0 . 1 mg Ir , cm − 2 ) may require the use of nanometer-sized MPLs with unsupported CLs or micrometer-sized MPLs with bimodal CLs. Furthermore, the decline of the volume reactive area at ultra-low Ir loading needs a maximization of the exchange current density and the specific electrochemical surface area, and a decrease of the catalyst oxygen coverage factor in the anode CL. • A 2D parametric analysis of key factors of the anode PTL/CL interface is presented • In-plane CL electrical resistance at PTL interface plays a critical role on performance. • Low Ir loading ( 0 . 1 mg Ir , cm − 2 ) can be achieved with micrometer-sized MPL or bimodal CL. • Ultra-low Ir loading ( ≲ 0 . 1 mg Ir , cm − 2 ) can be reached with fine MPLs and bimodal CL. • Optimization of volumetric exchange current density and gas saturation is needed.

Authors

Institutions

Publication Details

Journal
Chemical Engineering Journal
Published
2025-02-26
DOI
https://doi.org/10.1016/j.cej.2025.160722
Citations
11
Primary Topic
Hybrid Renewable Energy Systems
Type
article
Field-Weighted Citation Impact
5.85

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

The critical role of the anode porous transport layer/catalyst layer interface of polymer electrolyte membrane water electrolyzers: A parametric analysis

Jack Todd Lang, Yu Morimoto, Pablo A. García‐Salaberri, Iryna V. Zenyuk et al.
11 citations
Chemical Engineering Journal
Hybrid Renewable Energy Systems
5.85
article

The critical role of the anode porous transport layer/catalyst layer interface of polymer electrolyte membrane water electrolyzers: A parametric analysis

Jack Todd Lang, Yu Morimoto, Pablo A. García‐Salaberri, Iryna V. Zenyuk, Hung-Ming Chang, Nausir Firas, Hasan Shazhad
article en
11 citations

Abstract

Reducing the dependency of proton exchange membrane water electrolyzers (PEMWE) on precious metals, such as iridium (Ir), is necessary to develop a widespread green hydrogen system. This challenge requires a careful design of the interface between the anode porous transport layer (PTL) and the catalyst layer (CL). A comprehensive numerical analysis of relevant parameters that govern the behavior of the anode PTL/CL interface is presented. Calculations are also combined with an experimental characterization of the thickness and electrical conductivity of an unsupported CL as a function of Ir loading. The results show that the in-plane electrical resistance at the anode PTL/CL interface plays a critical role in cell performance. Reaching an acceptable electrical resistance at low Ir loading ( L Ir ≃ 0 . 1 mg Ir , cm − 2 ) can be accomplished through the incorporation of a micrometer-sized microporous layer (MPL) onto the PTL or the preparation of bimodal CLs with a secondary conductive phase. Further reduction of the Ir loading to the ultra-low regime ( L Ir ≲ 0 . 1 mg Ir , cm − 2 ) may require the use of nanometer-sized MPLs with unsupported CLs or micrometer-sized MPLs with bimodal CLs. Furthermore, the decline of the volume reactive area at ultra-low Ir loading needs a maximization of the exchange current density and the specific electrochemical surface area, and a decrease of the catalyst oxygen coverage factor in the anode CL. • A 2D parametric analysis of key factors of the anode PTL/CL interface is presented • In-plane CL electrical resistance at PTL interface plays a critical role on performance. • Low Ir loading ( 0 . 1 mg Ir , cm − 2 ) can be achieved with micrometer-sized MPL or bimodal CL. • Ultra-low Ir loading ( ≲ 0 . 1 mg Ir , cm − 2 ) can be reached with fine MPLs and bimodal CL. • Optimization of volumetric exchange current density and gas saturation is needed.

Chemical Engineering JournalVol. 509
Universidad Rey Juan Carlos (ES), University of California, Irvine (US), Universidad Carlos III de Madrid (ES)
Agencia Estatal de Investigación
Clean water and sanitation
Openalex Percentile: Top 4%
Hybrid Renewable Energy Systems
5.85
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.