Influence of Molecular Weight and Temperature on the Pyrolysis Behavior of Polyethylene
The pyrolysis technique is a useful recycling method for waste polyethylene (PE). Various PEs with different molecular weights have been produced and are widely used. The major pyrolysis products of PE include alkadienes (C<sub>n</sub>H<sub>2n-2</sub>), alkenes (C<sub>n</sub>H<sub>2n</sub>), and alkanes (C<sub>n</sub>H<sub>2n+2</sub>). In this study, the differences in pyrolysis behavior of PE based on its molecular weight and the pyrolysis temperature (423-764 °C) were investigated using four types of PEs, with M<sub>w</sub> = 2.0 × 10<sup>3</sup>, 16.0 × 10<sup>3</sup>, 28.3 × 10<sup>3</sup>, and 56.8 × 10<sup>3</sup> g/mol. More specifically, the pyrolysis products were compared in terms of their type (alkanes, alkenes, and alkadienes) and size (the number of carbon atoms). The order of production was alkenes > alkanes > alkadienes. The alkadiene/alkene ratios tended to increase with the PE molecular weight and size of the pyrolysis products. The alkadiene/alkene ratio increased until the pyrolysis temperature reached 670 °C. The alkane/alkene ratios tended to decrease as the PE molecular weight increased; however, they increased with the increasing size of the pyrolysis products. The alkane/alkene ratio decreased as the pyrolysis temperature increased, until it reached 670 °C. The formation of alkenes was more favorable than that of alkadienes and alkanes.
Authors
- Eunji Chae (ORCID: https://orcid.org/0000-0001-7486-7967)
- Sung-Seen Choi
Institutions
- Sejong University (KR)
Publication Details
- Journal
- Polymers
- Published
- 2025-02-21
- DOI
- https://doi.org/10.3390/polym17050576
- Citations
- 2
- Primary Topic
- Polymer crystallization and properties
- Type
- article
- Field-Weighted Citation Impact
- 1.21
Funders
- Ministry of Trade, Industry and Energy