Synthesis and Characterization of MO:ZnO/Fe<sub>2</sub>O<sub>3</sub> Nanocomposite and Its Effectiveness in the Degradation of Green Malachite Dye: Molecular Dynamics and Electronic Properties Study of Green Malachite Adsorption

Nanocomposites have attracted significant attention from researchers due to their remarkable chemical, adsorptive, and thermal properties. This work focuses on the synthesis of the montmorillonite modified with octadecylamine (MO):ZnO/Fe<sub>2</sub>O<sub>3</sub> (MO:ZnO/Fe<sub>2</sub>O<sub>3</sub>) nanocomposite. The ZnO/Fe<sub>2</sub>O<sub>3</sub> nanocomposite and MO were mixed in solution to create the component. XRD, FTIR, BET, TEM, MEB, and UV-vis were used to characterize the materials. In terms of their textural, morphological, and structural characteristics, interesting results were found. After 30 min of sunlight exposure, 96.12% of the GM dye can be degraded using just 0,02 g of MO:ZnO/Fe<sub>2</sub>O<sub>3</sub> (1:2(1/0.05)). In contrast, ZnO NPs exhibited the highest percentage of degradation under UV light, achieving 91.85%. The greater efficiency of MO:ZnO/Fe<sub>2</sub>O<sub>3</sub> under sunlight is attributed to its narrower band gap of 2.25 eV, which enables better utilization of visible light. Next using the Forcite and CASTEP modules in the Material Studio software, the GM dye's adsorption behavior on the surface of the as-prepared nanocomposite was analyzed. The results demonstrate that the GM/MO interaction is of the chemisorption type, predominantly governed by hydrogen bonding, electrostatic interactions, and π-π interactions between GM molecules. The ZnO (100) surface exhibits the highest density of active sites for GM degradation via a chemisorption adsorption process. Molecular dynamics simulations at 289.15 K reveal that the redox processes responsible for the degradation of the GM pollutant and its conversion into CO<sub>2</sub> gas are exothermic. For ZnO, the electronic properties yield a band gap of 2.686 eV. For GM/ZnO (100) and GM/ZnO (101), the band gaps were determined to be 0.291 and 2.704 eV, respectively, by using a 340 eV cutoff energy and the GGA RPBE pseudofunctional.

Authors

Institutions

Publication Details

Journal
Langmuir
Published
2025-02-20
DOI
https://doi.org/10.1021/acs.langmuir.4c04609
Citations
4
Primary Topic
Adsorption and biosorption for pollutant removal
Type
article
Field-Weighted Citation Impact
3.27
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Synthesis and Characterization of MO:ZnO/Fe2O3 Nanocomposite and Its Effectiveness in the Degradation of Green Malachite Dye: Molecular Dynamics and Electronic Properties Study of Green Malachite Adsorption

Rihem Jemai, Moez Hajji, Olfa Kamoun, Abdesslem Ben Haj Amara et al.
4 citations
Langmuir
Adsorption and biosorption for pollutant removal
3.27
article

Synthesis and Characterization of MO:ZnO/Fe2O3 Nanocomposite and Its Effectiveness in the Degradation of Green Malachite Dye: Molecular Dynamics and Electronic Properties Study of Green Malachite Adsorption

Rihem Jemai, Moez Hajji, Olfa Kamoun, Abdesslem Ben Haj Amara, Hafsia Ben Rhaiem, Z. Ahmed
article en
4 citations

Abstract

Nanocomposites have attracted significant attention from researchers due to their remarkable chemical, adsorptive, and thermal properties. This work focuses on the synthesis of the montmorillonite modified with octadecylamine (MO):ZnO/Fe<sub>2</sub>O<sub>3</sub> (MO:ZnO/Fe<sub>2</sub>O<sub>3</sub>) nanocomposite. The ZnO/Fe<sub>2</sub>O<sub>3</sub> nanocomposite and MO were mixed in solution to create the component. XRD, FTIR, BET, TEM, MEB, and UV-vis were used to characterize the materials. In terms of their textural, morphological, and structural characteristics, interesting results were found. After 30 min of sunlight exposure, 96.12% of the GM dye can be degraded using just 0,02 g of MO:ZnO/Fe<sub>2</sub>O<sub>3</sub> (1:2(1/0.05)). In contrast, ZnO NPs exhibited the highest percentage of degradation under UV light, achieving 91.85%. The greater efficiency of MO:ZnO/Fe<sub>2</sub>O<sub>3</sub> under sunlight is attributed to its narrower band gap of 2.25 eV, which enables better utilization of visible light. Next using the Forcite and CASTEP modules in the Material Studio software, the GM dye's adsorption behavior on the surface of the as-prepared nanocomposite was analyzed. The results demonstrate that the GM/MO interaction is of the chemisorption type, predominantly governed by hydrogen bonding, electrostatic interactions, and π-π interactions between GM molecules. The ZnO (100) surface exhibits the highest density of active sites for GM degradation via a chemisorption adsorption process. Molecular dynamics simulations at 289.15 K reveal that the redox processes responsible for the degradation of the GM pollutant and its conversion into CO<sub>2</sub> gas are exothermic. For ZnO, the electronic properties yield a band gap of 2.686 eV. For GM/ZnO (100) and GM/ZnO (101), the band gaps were determined to be 0.291 and 2.704 eV, respectively, by using a 340 eV cutoff energy and the GGA RPBE pseudofunctional.

LangmuirVol. 41(8)
Tunis University (TN), Kohat University of Science and Technology (PK), University of Carthage (TN), Tunis El Manar University (TN)
Openalex Percentile: Top 10%
Adsorption and biosorption for pollutant removal
3.27
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.