Defect Reduction and Line Width Roughness Improvement by Using a Post Precoat Treatment in Waferless Chamber Conditioning

Defect and line width roughness (LWR) are two main yield detractors in advanced plasma etch process in high-volume memory manufacturing. In this paper, we present the results of defect reduction and LWR improvement by using a post pre-coat treatment (PPT) method in waferless chamber clean (WCC) recipe. Adding a PPT step at the end of WCC recipe reduces defect, inline critical dimension (CD) variation and LWR. Atomic force microscopy (AFM) results show pre-coat silicon oxide and/or PPT improves surface roughness by 30%. X-ray photoelectron spectroscopy (XPS) has been utilized to characterize the surfaces treated with and without PPT, indicating PPT can remove residue chloride and solidify SiO2 film from its loose form. With the implementation of WCC with PPT, we have achieved yield improvement, which is attributed to defect reduction, tighter inline CD and LWR improvement.

Authors

Institutions

Publication Details

Journal
IEEE Transactions on Semiconductor Manufacturing
Published
2025-02-13
DOI
https://doi.org/10.1109/tsm.2025.3535145
Citations
1
Primary Topic
Advancements in Photolithography Techniques
Type
article
Field-Weighted Citation Impact
0.73
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Defect Reduction and Line Width Roughness Improvement by Using a Post Precoat Treatment in Waferless Chamber Conditioning

Fei Lu, Jeff J. Ye, Raviteja Pagadala
1 citations
IEEE Transactions on Semiconductor Manufacturing
Advancements in Photolithography Techniques
0.73
article

Defect Reduction and Line Width Roughness Improvement by Using a Post Precoat Treatment in Waferless Chamber Conditioning

Fei Lu, Jeff J. Ye, Raviteja Pagadala
article en
1 citations

Abstract

Defect and line width roughness (LWR) are two main yield detractors in advanced plasma etch process in high-volume memory manufacturing. In this paper, we present the results of defect reduction and LWR improvement by using a post pre-coat treatment (PPT) method in waferless chamber clean (WCC) recipe. Adding a PPT step at the end of WCC recipe reduces defect, inline critical dimension (CD) variation and LWR. Atomic force microscopy (AFM) results show pre-coat silicon oxide and/or PPT improves surface roughness by 30%. X-ray photoelectron spectroscopy (XPS) has been utilized to characterize the surfaces treated with and without PPT, indicating PPT can remove residue chloride and solidify SiO2 film from its loose form. With the implementation of WCC with PPT, we have achieved yield improvement, which is attributed to defect reduction, tighter inline CD and LWR improvement.

IEEE Transactions on Semiconductor ManufacturingVol. 38(3)
Micron (United States) (US), Intel (United States) (US), Cirrus Logic (United States) (US), Samsung (United States) (US), Université Bourgogne Franche-Comté (FR)
Openalex Percentile: Top 31%
Advancements in Photolithography Techniques
0.73
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.