Electron Ptychography for Atom-by-Atom Quantification of 1D Defect Complexes in Monolayer MoS<sub>2</sub>

Defect complexes can induce beneficial functionalities in two-dimensional (2D) semiconductors. However, understanding their formation mechanism with single-atom sensitivity has proven to be challenging for light elements using conventional transmission electron microscopy (TEM) techniques. Here, we demonstrate the atom-resolved formation of various one-dimensional (1D) defect complexes─consisting of rhenium dopants, sulfur interstitials, and sulfur vacancies─in monolayer MoS<sub>2</sub> by applying electron ptychography to our four-dimensional scanning transmission electron microscopy (4D-STEM) data sets. Our image resolution of 0.35 Å and a spatial precision of 2 pm allow us to achieve accurate matching between experimental structures and density functional theory (DFT) simulations at the atomic level. Additionally, we utilize out-of-focus ptychography to observe defect formation processes at dose rates comparable to those used in conventional TEM imaging, while maintaining a large field of view. This study demonstrates the systematic application of electron ptychography to extensive 4D-STEM data sets for quantitative defect imaging in 2D materials. We provide direct, atomically precise evidence that critical defect densities govern the formation of extended 1D defect complexes. For instance, we show that sulfur single-vacancy lines form when the vacancy density reaches 5 × 10<sup>13</sup> cm<sup>-2</sup> and transform into double-vacancy lines beyond 8 × 10<sup>13</sup> cm<sup>-2</sup>. Rhenium-dopant lines emerge at a dopant concentration higher than 3 × 10<sup>13</sup> cm<sup>-2</sup>, where metastable sulfur interstitial-vacancy lines also form as the cumulative electron dose reaches 3 × 10<sup>5</sup> e/Å<sup>2</sup>, initiating a local nucleation of the 1T' phase. Our results highlight the potential of electron ptychography for high-precision defect characterization and engineering in ultrathin 2D materials.

Authors

Institutions

Publication Details

Journal
ACS Nano
Published
2025-02-07
DOI
https://doi.org/10.1021/acsnano.4c14988
Citations
3
Primary Topic
Advanced Electron Microscopy Techniques and Applications
Type
article
Field-Weighted Citation Impact
7.65

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Electron Ptychography for Atom-by-Atom Quantification of 1D Defect Complexes in Monolayer MoS2

Michel Bosman, Daria Kieczka, Goki Eda, Leyi Loh et al.
3 citations
ACS Nano
Advanced Electron Microscopy Techniques and Applications
7.65
article

Electron Ptychography for Atom-by-Atom Quantification of 1D Defect Complexes in Monolayer MoS2

Michel Bosman, Daria Kieczka, Goki Eda, Leyi Loh, Alexander L. Shluger, Shoucong Ning, Yuan Chen, Yang Jian-min, Zhe Wang, Stephen J. Pennycook
article en
3 citations

Abstract

Defect complexes can induce beneficial functionalities in two-dimensional (2D) semiconductors. However, understanding their formation mechanism with single-atom sensitivity has proven to be challenging for light elements using conventional transmission electron microscopy (TEM) techniques. Here, we demonstrate the atom-resolved formation of various one-dimensional (1D) defect complexes─consisting of rhenium dopants, sulfur interstitials, and sulfur vacancies─in monolayer MoS<sub>2</sub> by applying electron ptychography to our four-dimensional scanning transmission electron microscopy (4D-STEM) data sets. Our image resolution of 0.35 Å and a spatial precision of 2 pm allow us to achieve accurate matching between experimental structures and density functional theory (DFT) simulations at the atomic level. Additionally, we utilize out-of-focus ptychography to observe defect formation processes at dose rates comparable to those used in conventional TEM imaging, while maintaining a large field of view. This study demonstrates the systematic application of electron ptychography to extensive 4D-STEM data sets for quantitative defect imaging in 2D materials. We provide direct, atomically precise evidence that critical defect densities govern the formation of extended 1D defect complexes. For instance, we show that sulfur single-vacancy lines form when the vacancy density reaches 5 × 10<sup>13</sup> cm<sup>-2</sup> and transform into double-vacancy lines beyond 8 × 10<sup>13</sup> cm<sup>-2</sup>. Rhenium-dopant lines emerge at a dopant concentration higher than 3 × 10<sup>13</sup> cm<sup>-2</sup>, where metastable sulfur interstitial-vacancy lines also form as the cumulative electron dose reaches 3 × 10<sup>5</sup> e/Å<sup>2</sup>, initiating a local nucleation of the 1T' phase. Our results highlight the potential of electron ptychography for high-precision defect characterization and engineering in ultrathin 2D materials.

ACS NanoVol. 19(6)
Agency for Science, Technology and Research (SG), University of Science and Technology of China (CN), National University of Singapore (SG), Tohoku University (JP), London Centre for Nanotechnology (GB), Institute of Materials Research and Engineering (SG), Centre of Excellence for Advanced Materials (CN), University of Chinese Academy of Sciences (CN), University College London (GB)
Agency for Science, Technology and Research, National Research Foundation Singapore, Ministry of Education - Singapore, Engineering and Physical Sciences Research Council
Openalex Percentile: Top 5%
Advanced Electron Microscopy Techniques and Applications
7.65
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.