Effect of surface conditioning on the adhesive bond strength of 3D-printed resins used in permanent fixed dental prostheses
Aluminium oxide increases the adhesive strength of 3D-printed dental restorative materials. Although the adhesive bond increased slightly with increasing airborne-particle abrasion pressure, the 3D restorative materials also exhibited an increased failure rate within the restorative material in the shear bond strength test with increasing blasting pressure.
Authors
- Arndt Guentsch (ORCID: https://orcid.org/0000-0001-8989-1441)
- Sándor Nietzsche (ORCID: https://orcid.org/0000-0002-1198-6464)
- Zaid Badr (ORCID: https://orcid.org/0000-0002-5638-3288)
- Stephanie Viebranz
- Marco Dederichs
- Ulrike Schulze‐Späte (ORCID: https://orcid.org/0000-0002-8046-0394)
- Anne-Sophie Schmelzer
- T Lehmann
Institutions
- Marquette University (US)
- Jena University Hospital (DE)
Publication Details
- Journal
- Journal of Dentistry
- Published
- 2025-02-07
- DOI
- https://doi.org/10.1016/j.jdent.2025.105621
- Citations
- 6
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 10.05