Measurement of crack width from the two-dimensional sonar images of the moss-covered surface of underwater concrete components based on K-means clustering

Imaging sonar can precisely measure the sizes of some large defects on the surface of underwater concrete components (UCCs). However, it is challenging for image sonar to measure the widths of small cracks on UCCs. Another difficulty is the coverage of aquatic organisms, such as moss. The moss coverage divided into four stages changes the hardness and roughness of UCCs to cause wrong signal intensity of echo, crack image generation, and crack width measurement. This article first illustrates the imaging principles of surficial cracks in UCCs using a two-dimensional imaging sonar and derives a theoretical equation of crack width measurement. Then, the appropriate settings of two main factors in actual inspection, scanning distance l and pitch angle α , are determined by experimentally obtaining the measurement error distribution of concrete cracks with various stages of moss coverage. It also summarizes the correction equation of crack width measurement at different stages of moss coverage. For the case of unknown stages of moss coverage, the peak gray P and the mean value M of fitting the Gaussian curve of the gray-level histogram of the sonar images are experimentally proved to be effective in distinguishing the different stages of moss coverage by a K-means clustering process. Experimental results indicate that 0.75 m ≤ l ≤ 2.0 m and 15° ≤ α ≤ 30° is the appropriate ranges of l and α in the practical measurement. The boundary line equation to separate Stage I and Stages II & III of moss coverage is 60 ≤ P + M ≤ 80. The boundary line equation to separate Stages II & III and Stage IV is 75 ≤ P + M ≤ 110.

Authors

Institutions

Publication Details

Journal
Structural Health Monitoring
Published
2024-12-30
DOI
https://doi.org/10.1177/14759217241302111
Citations
2
Primary Topic
Infrastructure Maintenance and Monitoring
Type
article
Field-Weighted Citation Impact
0.52
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Measurement of crack width from the two-dimensional sonar images of the moss-covered surface of underwater concrete components based on K-means clustering

Sheng Shen, Jianteng Chen, Zheng Cao, Zhidong Zheng et al.
2 citations
Structural Health Monitoring
Infrastructure Maintenance and Monitoring
0.52
article

Measurement of crack width from the two-dimensional sonar images of the moss-covered surface of underwater concrete components based on K-means clustering

Sheng Shen, Jianteng Chen, Zheng Cao, Zhidong Zheng, Chao Zhou, Mengli Zhang, Hong Zheng
article en
2 citations

Abstract

Imaging sonar can precisely measure the sizes of some large defects on the surface of underwater concrete components (UCCs). However, it is challenging for image sonar to measure the widths of small cracks on UCCs. Another difficulty is the coverage of aquatic organisms, such as moss. The moss coverage divided into four stages changes the hardness and roughness of UCCs to cause wrong signal intensity of echo, crack image generation, and crack width measurement. This article first illustrates the imaging principles of surficial cracks in UCCs using a two-dimensional imaging sonar and derives a theoretical equation of crack width measurement. Then, the appropriate settings of two main factors in actual inspection, scanning distance l and pitch angle α , are determined by experimentally obtaining the measurement error distribution of concrete cracks with various stages of moss coverage. It also summarizes the correction equation of crack width measurement at different stages of moss coverage. For the case of unknown stages of moss coverage, the peak gray P and the mean value M of fitting the Gaussian curve of the gray-level histogram of the sonar images are experimentally proved to be effective in distinguishing the different stages of moss coverage by a K-means clustering process. Experimental results indicate that 0.75 m ≤ l ≤ 2.0 m and 15° ≤ α ≤ 30° is the appropriate ranges of l and α in the practical measurement. The boundary line equation to separate Stage I and Stages II & III of moss coverage is 60 ≤ P + M ≤ 80. The boundary line equation to separate Stages II & III and Stage IV is 75 ≤ P + M ≤ 110.

Structural Health MonitoringVol. 25(2)
Analysis and Testing Centre (CN), China Communications Construction Company (China) (CN), Fuzhou University (CN)
Life below water
Openalex Percentile: Top 34%
Infrastructure Maintenance and Monitoring
0.52
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.