Effect of static magnetic field on microstructure and mechanical property of AlSi10Mg alloy by laser directed energy deposition

Laser directed energy deposition (LDED) is one of the popular metal additive manufacturing techniques. However, owing to the steep temperature gradient in melt pool, its as-built part is featured by coarse columnar crystal structures which is detrimental for the mechanical properties. This work uses an infrared laser with a wavelength of 960 nm to conduct the LDED process of AlSi10Mg alloy, where magnetic field with various intensities is employed to tailor the macroscopic morphology, microstructure and mechanical properties of the processed sample. The results show that with the static magnetic field, the melted single track becomes narrower and higher with a corresponding larger wetting angle, changing the stability and quality of layer-by-layer deposition. This can be attributed to the weakened outward Marangoni melt pool flow by the magnetic damping effect. When the magnetic field intensity goes from 0 to 0.2 T, the average grain size decreases from 58.1 μm to 44.1 μm. The magnetic field is effective in refining grain structures and promoting the columnar-to-equiaxed transition of LDED process, while its influence on fusion defects of pores is not remarkable. Due to the thermoelectric-magnetic effect, the volume force imposed on the dendrite is sufficient to fracture the dendrite arm and then reduce the dendrite spacing. In addition, the magnetic field can increase the elongation of AlSi10Mg alloy from 3.5 ± 0.2% to 5.5 ± 0.2% because of the refinement of the grains and the primary dendrite arm spacing. The study provides new insights into the potential of using magnetic field during LDED process to improve the microstructure and mechanical property of AlSi10Mg alloy. • The uniform magnetic field was used to modify the microstructure and mechanical property of LDED fabricated AliSi10Mg alloy. • The shape of the melt track changes with the magnetic field, which makes layer-by-layer deposition process easier. • New insights into the potential for using magnetic field during LDED and adding material performance benefits.

Authors

Institutions

Publication Details

Journal
Journal of Materials Research and Technology
Published
2024-12-27
DOI
https://doi.org/10.1016/j.jmrt.2024.12.237
Citations
7
Primary Topic
Additive Manufacturing Materials and Processes
Type
article
Field-Weighted Citation Impact
1.49
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of static magnetic field on microstructure and mechanical property of AlSi10Mg alloy by laser directed energy deposition

Weiming Niu, Jiasen Han, Haiou Yang, Hui Chen et al.
7 citations
Journal of Materials Research and Technology
Additive Manufacturing Materials and Processes
1.49
article

Effect of static magnetic field on microstructure and mechanical property of AlSi10Mg alloy by laser directed energy deposition

Weiming Niu, Jiasen Han, Haiou Yang, Hui Chen, Zhifu Yao, Xin Lin, Bingke Song
article en
7 citations

Abstract

Laser directed energy deposition (LDED) is one of the popular metal additive manufacturing techniques. However, owing to the steep temperature gradient in melt pool, its as-built part is featured by coarse columnar crystal structures which is detrimental for the mechanical properties. This work uses an infrared laser with a wavelength of 960 nm to conduct the LDED process of AlSi10Mg alloy, where magnetic field with various intensities is employed to tailor the macroscopic morphology, microstructure and mechanical properties of the processed sample. The results show that with the static magnetic field, the melted single track becomes narrower and higher with a corresponding larger wetting angle, changing the stability and quality of layer-by-layer deposition. This can be attributed to the weakened outward Marangoni melt pool flow by the magnetic damping effect. When the magnetic field intensity goes from 0 to 0.2 T, the average grain size decreases from 58.1 μm to 44.1 μm. The magnetic field is effective in refining grain structures and promoting the columnar-to-equiaxed transition of LDED process, while its influence on fusion defects of pores is not remarkable. Due to the thermoelectric-magnetic effect, the volume force imposed on the dendrite is sufficient to fracture the dendrite arm and then reduce the dendrite spacing. In addition, the magnetic field can increase the elongation of AlSi10Mg alloy from 3.5 ± 0.2% to 5.5 ± 0.2% because of the refinement of the grains and the primary dendrite arm spacing. The study provides new insights into the potential of using magnetic field during LDED process to improve the microstructure and mechanical property of AlSi10Mg alloy. • The uniform magnetic field was used to modify the microstructure and mechanical property of LDED fabricated AliSi10Mg alloy. • The shape of the melt track changes with the magnetic field, which makes layer-by-layer deposition process easier. • New insights into the potential for using magnetic field during LDED and adding material performance benefits.

Journal of Materials Research and TechnologyVol. 34
Northwestern Polytechnical University (CN), Shanghai Academy of Spaceflight Technology (CN)
Affordable and clean energy
Openalex Percentile: Top 19%
Additive Manufacturing Materials and Processes
1.49
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.