Stress-strain properties of microwave-irradiated polymer composite based on PDI-3A rubber
The stress diagram of polymer composite material based on PDI-3A rubber filled with thermally expanded graphite or potassium chloride before and after microwave treatment for 300, 600, 900 and 1200 s has been studied. A twofold increase in tensile strength and deformability was found after microwave treatment for 300 c and testing at 223 K. With increasing the test temperature or microwave treatment time, a marked decrease in the deformation and tensile strength characteristics of the obtained composites was observed.
Authors
- А. Н. Козлов (ORCID: https://orcid.org/0000-0002-6242-0911)
- Э. М. Нуруллаев
- Л. Л. Хименко
- S. R. Allayarov (ORCID: https://orcid.org/0000-0003-4096-6750)
Institutions
- Perm National Research Polytechnic University (RU)
- Perm State Agricultural Academy (RU)
Publication Details
- Journal
- Химия высоких энергий
- Published
- 2024-12-26
- DOI
- https://doi.org/10.31857/s0023119324040019
- Primary Topic
- Synthesis of Tetrazole Derivatives
- Type
- article
- Field-Weighted Citation Impact