Photofunctionalized Europium(III) complexes with circularly polarized luminescence

Europium(III) complexes that emit circularly polarized light (CPL) have potential applications in various fields, including bioimaging, sensing, and optoelectronic devices. This study investigates the synthesis and characterization of europium(III) complexes having CPL activity by incorporating chiral ligand (+)-3-(trifluoroacetyl)camphor (tfc) and triphenylene diphenylphosphine oxide (DPO) ligands . The europium acetate salt was converted to europium trifluoroacetyl camphorate ([Eu(tfc) 3 )(H 2 O)]) in the 1st step of the four-step synthesis reaction. In the 2nd step chlorodiphenylphosphine and 6-bromotriphenylene in the presence of the catalyst n-BuLi at -80 °C in dry THF solvent produce triphenylene phosphine ligand. In the 3rd step of the synthesis process, the synthesized triphenylene diphenyl phosphine undergoes oxidation to phosphine oxide, DPO using hydrogen peroxide (H 2 O 2 ) as a catalyst at a low temperature of 0 °C. In the final and fourth step of the chiro optical europium complex synthesis, [Eu(tfc) 3 (DPO) 2 ](H 2 O) 2 was prepared by reacting the previously synthesized DPO ligand with [Eu(tfc) 3 ](H 2 O) 2 in dichloromethane solvent at room temperature for a duration of three hours. The NMR, FTIR, Elemental analysis, TGA and powder XRD confirmed the proposed molecular formula C66H70F9O6EuP. Upon excitation at 375 nm, the complex displayed characteristic sharp emission peaks in the visible region emission bands which were observed at 580, 595, 614, 652, and 703 nm, corresponding to the 4f-4f transitions of the Eu(III) ion. The high intensity ratio of 5 D 0 – 7 F 2 to 5 D 0 – 7 F 1 indicated a non-centrosymmetric ligand arrangement. The synthesized complex displayed significant circularly polarized luminescence (CPL) properties, exhibiting an absolute g CPL value of 0.025 and an absolute quantum yield of 4.09 %. With a 8 % sensitization efficiency and a 0.56 ms photoluminescent lifetime, this complex shows promise for potential applications in optoelectronic devices and chiral sensing. The challenges such as back energy transfer and structural stability limited the overall luminescence efficiency.

Authors

Institutions

Publication Details

Journal
Chemical Physics Impact
Published
2024-12-24
DOI
https://doi.org/10.1016/j.chphi.2024.100806
Citations
4
Primary Topic
Lanthanide and Transition Metal Complexes
Type
article
Field-Weighted Citation Impact
0.47

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Photofunctionalized Europium(III) complexes with circularly polarized luminescence

Naima Sharmin, Md. Jahidul Islam
4 citations
Chemical Physics Impact
Lanthanide and Transition Metal Complexes
0.47
article

Photofunctionalized Europium(III) complexes with circularly polarized luminescence

Naima Sharmin, Md. Jahidul Islam
article en
4 citations

Abstract

Europium(III) complexes that emit circularly polarized light (CPL) have potential applications in various fields, including bioimaging, sensing, and optoelectronic devices. This study investigates the synthesis and characterization of europium(III) complexes having CPL activity by incorporating chiral ligand (+)-3-(trifluoroacetyl)camphor (tfc) and triphenylene diphenylphosphine oxide (DPO) ligands . The europium acetate salt was converted to europium trifluoroacetyl camphorate ([Eu(tfc) 3 )(H 2 O)]) in the 1st step of the four-step synthesis reaction. In the 2nd step chlorodiphenylphosphine and 6-bromotriphenylene in the presence of the catalyst n-BuLi at -80 °C in dry THF solvent produce triphenylene phosphine ligand. In the 3rd step of the synthesis process, the synthesized triphenylene diphenyl phosphine undergoes oxidation to phosphine oxide, DPO using hydrogen peroxide (H 2 O 2 ) as a catalyst at a low temperature of 0 °C. In the final and fourth step of the chiro optical europium complex synthesis, [Eu(tfc) 3 (DPO) 2 ](H 2 O) 2 was prepared by reacting the previously synthesized DPO ligand with [Eu(tfc) 3 ](H 2 O) 2 in dichloromethane solvent at room temperature for a duration of three hours. The NMR, FTIR, Elemental analysis, TGA and powder XRD confirmed the proposed molecular formula C66H70F9O6EuP. Upon excitation at 375 nm, the complex displayed characteristic sharp emission peaks in the visible region emission bands which were observed at 580, 595, 614, 652, and 703 nm, corresponding to the 4f-4f transitions of the Eu(III) ion. The high intensity ratio of 5 D 0 – 7 F 2 to 5 D 0 – 7 F 1 indicated a non-centrosymmetric ligand arrangement. The synthesized complex displayed significant circularly polarized luminescence (CPL) properties, exhibiting an absolute g CPL value of 0.025 and an absolute quantum yield of 4.09 %. With a 8 % sensitization efficiency and a 0.56 ms photoluminescent lifetime, this complex shows promise for potential applications in optoelectronic devices and chiral sensing. The challenges such as back energy transfer and structural stability limited the overall luminescence efficiency.

Chemical Physics ImpactVol. 10
International University of Business Agriculture and Technology (BD)
Ministry of Education, Culture, Sports, Science and Technology, Hokkaido University
Openalex Percentile: Top 37%
Lanthanide and Transition Metal Complexes
0.47
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.