Evaluating fatigue resistance in occlusal veneers: a comparative study of processing techniques and material thickness of lithium disilicate (IPS e.max Press vs. IPS e.max CAD)
At 0.5 mm or 0.8 mm material thickness, the processing technique did not affect the fatigue resistance or crack patterns of the lithium disilicate occlusal veneers. However, the lithium disilicate with a thickness of 0.8 mm exhibited a superior survival probability compared to that with a thickness of 0.5 mm.
Authors
- Daraporn Sae‐Lee (ORCID: https://orcid.org/0000-0001-5191-6068)
- Tanapon Sornsuwan (ORCID: https://orcid.org/0000-0002-5611-9436)
- Pokpong Amornvit (ORCID: https://orcid.org/0000-0001-7749-676X)
- Pimduen Rungsiyakull (ORCID: https://orcid.org/0000-0002-7497-6618)
- Pisaisit Chaijareenont
- Walisa Charoenporn
Institutions
- Khon Kaen University (TH)
- Bangkok Hospital (TH)
- Chiang Mai University (TH)
- Naresuan University (TH)
Publication Details
- Journal
- BMC Oral Health
- Published
- 2024-12-23
- DOI
- https://doi.org/10.1186/s12903-024-05347-7
- Citations
- 3
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 1.21
Funders
- Chiang Mai University