Highly efficient and selective aqueous phase hydrogenolysis of furfural to 1,5-pentanediol using bimetallic Ru–SnO<sub><i>x</i></sub>/γ-Al<sub>2</sub>O<sub>3</sub> catalysts
The presence of Ru 3 Sn 7 alloy phases and Ru 0 –SnO x species on the surface of γ-Al 2 O 3 can synergistically activate and hydrogenolyse the furan ring, producing a high yield of 1,5-PeD (up to 94%) at 180 °C, under H 2 = 30 bar and after reacting for 7 h.
Authors
- Kiky Corneliasari Sembiring (ORCID: https://orcid.org/0000-0003-1493-4165)
- Rodiansono Rodiansono (ORCID: https://orcid.org/0000-0002-9047-3586)
- Atina Sabila Azzahra
- Uripto Trisno Santoso (ORCID: https://orcid.org/0000-0003-1832-2596)
- Gagus Ketut Sunnardianto (ORCID: https://orcid.org/0000-0002-2781-0076)
- Edi Mikrianto
- Eka Suarso (ORCID: https://orcid.org/0000-0001-9867-7578)
- Indri Badria Adilina (ORCID: https://orcid.org/0000-0002-8700-1414)
- Ahmad Afandi
Institutions
- Surya University (ID)
- Indonesian Institute of Sciences (ID)
- Institute of Catalysis and Petrochemistry (RU)
- Lambung Mangkurat University (ID)
Publication Details
- Journal
- Catalysis Science & Technology
- Published
- 2024-12-20
- DOI
- https://doi.org/10.1039/d4cy01138d
- Citations
- 8
- Primary Topic
- Catalysis for Biomass Conversion
- Type
- article
- Field-Weighted Citation Impact
- 1.48