Research on the Design of Fluoride‐Free Continuous Casting Mold Flux System for High‐Aluminum Steel

To get rid of the restrictions imposed by the components of the original mold flux and minimize fluorides to the largest extent, this article has designed the continuous casting mold flux for high‐aluminum steel with an aluminum content of 1.35% and tested the performance manifestations of the mold flux by integrating equipment like a rotational viscometer, S/DHTT‐TA‐III thermal analyzer, and X‐ray diffraction. The composition of the continuous casting mold flux for high‐aluminum steel is: CaO = 23–43 wt%, SiO 2 = 12–25 wt%, Al 2 O 3 = 14–26 wt%, B 2 O 3 = 13–17 wt%, and Li 2 O = 4–8 wt%. The newly designed mold flux has a lower melting temperature and its performance still satisfies the conditions for continuous casting after the reaction. The crystallization process of the on‐site using mold flux lasts 198 s, with the precipitated phases being Na 2 CaSiO 4 and Ca 3 Si 2 O 7 . The crystallization process of the newly designed mold flux lasts ≈324 s, with the precipitated phase mainly being LiAlO 2 , and the mold flux can maintain a low viscosity and a relatively thick liquid slag layer for a longer period of time.

Authors

Institutions

Publication Details

Journal
steel research international
Published
2024-12-19
DOI
https://doi.org/10.1002/srin.202400786
Primary Topic
Metallurgical Processes and Thermodynamics
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Research on the Design of Fluoride‐Free Continuous Casting Mold Flux System for High‐Aluminum Steel

Hongbo Zeng, Rui Guan, Kang Yang, Xingang Ai
1 links
steel research international
Metallurgical Processes and Thermodynamics
article

Research on the Design of Fluoride‐Free Continuous Casting Mold Flux System for High‐Aluminum Steel

Hongbo Zeng, Rui Guan, Kang Yang, Xingang Ai
article en

Abstract

To get rid of the restrictions imposed by the components of the original mold flux and minimize fluorides to the largest extent, this article has designed the continuous casting mold flux for high‐aluminum steel with an aluminum content of 1.35% and tested the performance manifestations of the mold flux by integrating equipment like a rotational viscometer, S/DHTT‐TA‐III thermal analyzer, and X‐ray diffraction. The composition of the continuous casting mold flux for high‐aluminum steel is: CaO = 23–43 wt%, SiO 2 = 12–25 wt%, Al 2 O 3 = 14–26 wt%, B 2 O 3 = 13–17 wt%, and Li 2 O = 4–8 wt%. The newly designed mold flux has a lower melting temperature and its performance still satisfies the conditions for continuous casting after the reaction. The crystallization process of the on‐site using mold flux lasts 198 s, with the precipitated phases being Na 2 CaSiO 4 and Ca 3 Si 2 O 7 . The crystallization process of the newly designed mold flux lasts ≈324 s, with the precipitated phase mainly being LiAlO 2 , and the mold flux can maintain a low viscosity and a relatively thick liquid slag layer for a longer period of time.

steel research internationalVol. 96(7)
University of Science and Technology Liaoning (CN)
National Natural Science Foundation of China
Openalex Percentile: Top 76%
Metallurgical Processes and Thermodynamics
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.