Luminescence of bound excitons created near sodium impurity ions in KCl:Na single crystals

The study is focused on luminescence features of bound excitons (exciton-like formations, ELFs) in KCl:Na single crystals created in the field of sodium impurity ions either directly at photoexcitation or via the recombination of electron-hole pairs. The intensity of the X-ray luminescence (XRL) bands peaked at 2.8 and 3.1 eV (emission of recombinationally formed and relaxed ELFs) increases with both, the concentration of sodium impurity ions (10 → 1000 ppm) and the detection temperature (85 → 350 K). It is worth noting that at room temperature, the light yield of these XRL bands in KCl:Na practically coincides with that for the luminescence measured in the same way in classical scintillators, CsI and CsI:Na crystals. The lifetime of the fast component of cathodoluminescence at 2.8 and 3.1 eV equals 2.4 and 1.7 ns, respectively, at 6 K and even shortens to approximately τ ≈ 0.3 ns at room temperature. At 10 K, photons of 7.6 and 6.7 eV directly form ELFs in the field of single or paired Na + impurity ions with typical luminescence bands peaked, respectively, at 2.8 eV ( e l 0 (Na + )) and 3.1 eV ( e l 0 (Na + -Na + )). These photoluminescence bands undergo complete thermal quenching by 200–300 K, whereas relevant XRL bands are not quenched up to 350 K, their intensity even noticeably increases at 200 → 350 K. • Luminescence of bound excitons formed in KCl:Na directly or via e-h recombination. • X-ray exciton-like emission increases with both sodium concentration and temperature. • Emission of photocreated excitons is fully quenched while relevant XRL remains at RT.

Authors

Institutions

Publication Details

Journal
Optical Materials X
Published
2024-12-18
DOI
https://doi.org/10.1016/j.omx.2024.100395
Primary Topic
Luminescence Properties of Advanced Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Luminescence of bound excitons created near sodium impurity ions in KCl:Na single crystals

Kuanyshbek Shunkeyev, А. Tilep, Daulet Sergeyev, V. Nagirnyi et al.
Optical Materials X
Luminescence Properties of Advanced Materials
article

Luminescence of bound excitons created near sodium impurity ions in KCl:Na single crystals

Kuanyshbek Shunkeyev, А. Tilep, Daulet Sergeyev, V. Nagirnyi, Zh. Ubaev, Sh. Sagimbaeva, А. Krasnikov, A. Lushchik, Adelya Kenzhebayeva
article en

Abstract

The study is focused on luminescence features of bound excitons (exciton-like formations, ELFs) in KCl:Na single crystals created in the field of sodium impurity ions either directly at photoexcitation or via the recombination of electron-hole pairs. The intensity of the X-ray luminescence (XRL) bands peaked at 2.8 and 3.1 eV (emission of recombinationally formed and relaxed ELFs) increases with both, the concentration of sodium impurity ions (10 → 1000 ppm) and the detection temperature (85 → 350 K). It is worth noting that at room temperature, the light yield of these XRL bands in KCl:Na practically coincides with that for the luminescence measured in the same way in classical scintillators, CsI and CsI:Na crystals. The lifetime of the fast component of cathodoluminescence at 2.8 and 3.1 eV equals 2.4 and 1.7 ns, respectively, at 6 K and even shortens to approximately τ ≈ 0.3 ns at room temperature. At 10 K, photons of 7.6 and 6.7 eV directly form ELFs in the field of single or paired Na + impurity ions with typical luminescence bands peaked, respectively, at 2.8 eV ( e l 0 (Na + )) and 3.1 eV ( e l 0 (Na + -Na + )). These photoluminescence bands undergo complete thermal quenching by 200–300 K, whereas relevant XRL bands are not quenched up to 350 K, their intensity even noticeably increases at 200 → 350 K. • Luminescence of bound excitons formed in KCl:Na directly or via e-h recombination. • X-ray exciton-like emission increases with both sodium concentration and temperature. • Emission of photocreated excitons is fully quenched while relevant XRL remains at RT.

Optical Materials XVol. 25
Aktobe Regional State University named after K.Zhubanov (KZ), University of Tartu (EE)
Ministry of Education and Science of the Republic of Kazakhstan
Openalex Percentile: Top 85%
Luminescence Properties of Advanced Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.