Preparation and luminescence properties of Sr2SiO4 doped with Eu2+
Series concentration of Eu<sup>2+</sup> doped Sr<sub>2</sub>SiO<sub>4</sub> were synthesized by traditional high temperature solid method. The phase and luminescence properties of the phosphors were characterized by X-ray diffractometer (XRD) and fluorescence spectrophotometer. The analysis results show that the XRD patterns of phosphors were consistent with Sr<sub>2</sub>SiO<sub>4</sub> standard card PDF No.39-1256, illustrated no impurity phase was generated. The luminescence intensity of the phosphors increases first and then decrease with increasing of concentration (molar fraction) of Eu<sup>2+</sup>, when the Eu<sup>2+</sup> doped concentration is 4%, the luminescence intensity of phosphors is the strongest. The quenching mechanism of phosphors is further studied, the analysis results showed that the quenching mechanism is electric dipole-electric dipole interaction. With increasing of ventilation rate, the luminescence color of the phosphors gradually transitions from blue-green to yellow.
Authors
- Mei‐Hwan Wu (ORCID: https://orcid.org/0000-0002-7074-8087)
- Hongbo Zhu (ORCID: https://orcid.org/0009-0002-3229-0260)
- Wei Wang (ORCID: https://orcid.org/0000-0002-9263-7927)
Institutions
- China University of Petroleum, Beijing (CN)
- Karamay Central Hospital (CN)
Publication Details
- Published
- 2024-12-12
- DOI
- https://doi.org/10.1117/12.3052612
- Primary Topic
- Luminescence Properties of Advanced Materials
- Type
- article
- Field-Weighted Citation Impact
- 0.00