Effect of Temperature Gradient and Cooling Rate on the Solidification of Iron: A Molecular Dynamics Study

In this study, molecular dynamics (MD) simulations were employed to compare the effects of different solidification conditions on the solidification behaviour, stress distribution, and degree of crystallization of iron. The results indicate significant differences in nucleation and microstructural evolution between the two solidification methods. In the homogeneous temperature field, the solidification of iron is characterized by instantaneous nucleation. The BCC phase surged at 1431 K followed by the phenomenon of latent heat of crystallization. As the temperature continued to decrease, the percentage of the BCC phase continued to increase steadily. Eventually, the atoms aggregated to form a crystal nucleus and grow outward to form polycrystalline structures. During gradient solidification, continuous nucleation of iron leads to a slow increase in the BCC phase. From the initial stage of solidification, the solid-liquid interface moves in the direction of higher temperature and is accompanied by a higher stress distribution. Furthermore, increasing the temperature gradient, particularly the cooling rate, accelerates the transformation efficiency of iron in the gradient solidification process. In addition, increasing the cooling rate or temperature gradient reduces the residual stress and crystallinity of the solidified microstructure. It is worth noting that an increased temperature gradient or cooling rate will produce higher residual stress and uneven microstructure in the boundary region. This study provides an atomic-level understanding of the improvement in the solidification performance of iron.

Authors

Institutions

Publication Details

Journal
Materials
Published
2024-12-11
DOI
https://doi.org/10.3390/ma17246051
Citations
5
Primary Topic
Microstructure and mechanical properties
Type
article
Field-Weighted Citation Impact
0.59

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of Temperature Gradient and Cooling Rate on the Solidification of Iron: A Molecular Dynamics Study

Weizhuang Li, Lu Xie, Qin Qin, Dongyue Li et al.
5 citations
Materials
Microstructure and mechanical properties
0.59
article

Effect of Temperature Gradient and Cooling Rate on the Solidification of Iron: A Molecular Dynamics Study

Weizhuang Li, Lu Xie, Qin Qin, Dongyue Li, Wenrui Wang
article en
5 citations

Abstract

In this study, molecular dynamics (MD) simulations were employed to compare the effects of different solidification conditions on the solidification behaviour, stress distribution, and degree of crystallization of iron. The results indicate significant differences in nucleation and microstructural evolution between the two solidification methods. In the homogeneous temperature field, the solidification of iron is characterized by instantaneous nucleation. The BCC phase surged at 1431 K followed by the phenomenon of latent heat of crystallization. As the temperature continued to decrease, the percentage of the BCC phase continued to increase steadily. Eventually, the atoms aggregated to form a crystal nucleus and grow outward to form polycrystalline structures. During gradient solidification, continuous nucleation of iron leads to a slow increase in the BCC phase. From the initial stage of solidification, the solid-liquid interface moves in the direction of higher temperature and is accompanied by a higher stress distribution. Furthermore, increasing the temperature gradient, particularly the cooling rate, accelerates the transformation efficiency of iron in the gradient solidification process. In addition, increasing the cooling rate or temperature gradient reduces the residual stress and crystallinity of the solidified microstructure. It is worth noting that an increased temperature gradient or cooling rate will produce higher residual stress and uneven microstructure in the boundary region. This study provides an atomic-level understanding of the improvement in the solidification performance of iron.

MaterialsVol. 17(24)
University of Science and Technology Beijing (CN)
National Natural Science Foundation of China, China Postdoctoral Science Foundation, National Key Research and Development Program of China
Openalex Percentile: Top 32%
Microstructure and mechanical properties
0.59
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.