Impact of Silicon Impurity on the Hydrometallurgical Recovery of NCM622 Cathode

Hydrometallurgy is one of the best approaches to date for recycling LIBs due to its high efficiency, low energy usage, and industrial scalability. However, impurities have always been a thorny issue because they could have unintended impacts on the recovered cathode materials. This research marks the first systematic investigation into the influence of silicon impurity on the LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622) cathode obtained from hydrometallurgical recycling. We find that silicon nanoparticles will be nucleated at the center of the precursor particles during co-precipitation synthesis, and the silicon core will slowly dissolve in the surrounding ammonia, creating a special hollow structure in the particle. More importantly, the dissolution of silicon impurity will eventually lead to the deposition of silicates in the cathode material, which is an unfavorable result. Test data indicate that NCM622 cathode with 5 at% silicon has a capacity of 148.8 mAh g −1 after 100 cycles at 1/3 C, approximately 10 mAh g −1 lower than the virgin. Despite being relatively mild, the adverse influence of silicon impurity in hydrometallurgical recycling still requires attention.

Authors

Publication Details

Journal
Journal of The Electrochemical Society
Published
2024-12-03
DOI
https://doi.org/10.1149/1945-7111/ad9ccd
Citations
2
Primary Topic
Extraction and Separation Processes
Type
article
Field-Weighted Citation Impact
0.43

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Impact of Silicon Impurity on the Hydrometallurgical Recovery of NCM622 Cathode

Yadong Zheng, Yan Wang, Zhenzhen Yang
2 citations
Journal of The Electrochemical Society
Extraction and Separation Processes
0.43
article

Impact of Silicon Impurity on the Hydrometallurgical Recovery of NCM622 Cathode

Yadong Zheng, Yan Wang, Zhenzhen Yang
article en
2 citations

Abstract

Hydrometallurgy is one of the best approaches to date for recycling LIBs due to its high efficiency, low energy usage, and industrial scalability. However, impurities have always been a thorny issue because they could have unintended impacts on the recovered cathode materials. This research marks the first systematic investigation into the influence of silicon impurity on the LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622) cathode obtained from hydrometallurgical recycling. We find that silicon nanoparticles will be nucleated at the center of the precursor particles during co-precipitation synthesis, and the silicon core will slowly dissolve in the surrounding ammonia, creating a special hollow structure in the particle. More importantly, the dissolution of silicon impurity will eventually lead to the deposition of silicates in the cathode material, which is an unfavorable result. Test data indicate that NCM622 cathode with 5 at% silicon has a capacity of 148.8 mAh g −1 after 100 cycles at 1/3 C, approximately 10 mAh g −1 lower than the virgin. Despite being relatively mild, the adverse influence of silicon impurity in hydrometallurgical recycling still requires attention.

Journal of The Electrochemical SocietyVol. 171(12)
U.S. Department of Energy
Affordable and clean energy
Openalex Percentile: Top 40%
Extraction and Separation Processes
0.43
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.