Cement layer thickness and load-bearing capacity of tooth restored with lithium-disilicate glass ceramic and hybrid ceramic occlusal veneers
Within the limitations of this study, it can be concluded that thin HC occlusal veneers provided higher load-bearing capacity than LDGC counterparts of the same thickness. HC veneers were also less sensitive to the effect of cement layer thickness.