Two-stage firing of wear-resistant products of complex configuration made of aluminum-zirconium ceramics
The modes of two-stage firing of wear-resistant products of complex configuration made of aluminum-zirconium ceramics are described. The firing mode of ceramics in the first stage is carried out in air at a maximum temperature of 1500 oC with isothermal exposures of 2 and 8 hours at 1300 and 1500 oC, respectively. At the second stage, the method of hot isostatic pressing (НIР) was used at a maximum temperature of 1490 °C with a short-term exposure of 1 hour. The established modes of two-stage firing ensure the production of aluminum zirconium ceramics with a fine-grained structure (0.5‒2.5 microns), a relative density of 99.3 %, with a high level of physical and mechanical properties and resistance to aging.
Authors
- E. S. Semantsova
- П. М. Плетнев (ORCID: https://orcid.org/0000-0003-0190-7133)
Publication Details
- Journal
- NOVYE OGNEUPORY (NEW REFRACTORIES)
- Published
- 2024-12-03
- DOI
- https://doi.org/10.17073/1683-4518-2024-7-61-66
- Primary Topic
- Advanced ceramic materials synthesis
- Type
- article
- Field-Weighted Citation Impact
- 0.00