Effect of carbonate and silicate on the microstructural properties of the MgO-activated slag binder

MgO-based cementitious materials are an important direction of green, low-carbon and sustainable cementitious materials. This paper investigates the hydration characteristics of MgO-activated slag binder under the influence of carbonate and silicate. The results show that the combination of silica fume and Na 2 CO 3 is more effective in obtaining lower pore structure and refining microstructure than using silica fume or Na 2 CO 3 alone. The pore volume (<1000 nm) of the MgO-activated slag binder curing for 28d is reduced by nearly 80% compared with 3d. The addition of the small amount of SF reduces the content of bulk crystalline hydrotalcite and the content of bound and interlayer water in the gelling phase and promotes the generation of M-S-H gel phase. Controlling the type and content of multiple carbonates and silicate gel phases in preparing MgO-aluminosilicates binder can achieve better results in reducing the pore volume, refining the pore structure, and increasing the compressive strength.

Authors

Institutions

Publication Details

Journal
Open Ceramics
Published
2024-12-01
DOI
https://doi.org/10.1016/j.oceram.2024.100715
Citations
1
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.26
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of carbonate and silicate on the microstructural properties of the MgO-activated slag binder

Xinhua Yuan, Guangxue Liu, Jialong Wu, Hongqiang Ma et al.
1 citations
Open Ceramics
Concrete and Cement Materials Research
0.26
article

Effect of carbonate and silicate on the microstructural properties of the MgO-activated slag binder

Xinhua Yuan, Guangxue Liu, Jialong Wu, Hongqiang Ma, Enyang Dai, Jingjing Feng
article en
1 citations

Abstract

MgO-based cementitious materials are an important direction of green, low-carbon and sustainable cementitious materials. This paper investigates the hydration characteristics of MgO-activated slag binder under the influence of carbonate and silicate. The results show that the combination of silica fume and Na 2 CO 3 is more effective in obtaining lower pore structure and refining microstructure than using silica fume or Na 2 CO 3 alone. The pore volume (<1000 nm) of the MgO-activated slag binder curing for 28d is reduced by nearly 80% compared with 3d. The addition of the small amount of SF reduces the content of bulk crystalline hydrotalcite and the content of bound and interlayer water in the gelling phase and promotes the generation of M-S-H gel phase. Controlling the type and content of multiple carbonates and silicate gel phases in preparing MgO-aluminosilicates binder can achieve better results in reducing the pore volume, refining the pore structure, and increasing the compressive strength.

Open CeramicsVol. 21
Hebei University (CN), Shandong Agricultural University (CN)
Openalex Percentile: Top 43%
Concrete and Cement Materials Research
0.26
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.