Hydrometallurgical Processing of Antimony Bearing Pyrometallurgical Calcines
The solid pyrometallurgical calcination product containing antimony was dissolved in H2 SO4 under conditions that ensured a high extraction of the oxidized antimony compounds into the solution. The key conditions were [H2 SO4 ]-180 g/l, duration - 2 hours, temperature - 80 ºС, T: J = 1:6, and a rotation speed of 400-450 rpm. The study determined a high degree of antimony dissolution is possible and found the optimal points for the proposed process.
Authors
- Corby Anderson (ORCID: https://orcid.org/0000-0003-0193-2208)
Publication Details
- Published
- 2024-11-18
- DOI
- https://doi.org/10.54026/jmms/1095
- Primary Topic
- Metal Extraction and Bioleaching
- Type
- article
- Field-Weighted Citation Impact
- 0.00