Internal Fit and Marginal Adaptation of Posterior CAD/CAM Crowns Fabricated from Fully Crystallized Lithium Disilicate Compared to Partially Crystallized Lithium Disilicate with Two Finish Line Thicknesses: An In Vitro Study
GC Initial Lisi produced comparable results to the gold standard IPS e.max CAD, thus it can be used due to its clinically acceptable internal fit and marginal adaptation. How to cite this article: ElGendy M, Sherif R, Rabie K. Internal Fit and Marginal Adaptation of Posterior CAD/CAM Crowns Fabricated from Fully Crystallized Lithium Disilicate Compared to Partially Crystallized Lithium Disilicate with Two Finish Line Thicknesses: An <i>In Vitro</i> Study. J Contemp Dent Pract 2024;25(8):740-744.
Authors
- Rana Sherif (ORCID: https://orcid.org/0000-0003-3033-4100)
- Mohamed Hussein Elgendy (ORCID: https://orcid.org/0000-0001-9996-5344)
Institutions
- Badr University in Cairo (EG)
- Misr International University (EG)
Publication Details
- Journal
- The Journal of Contemporary Dental Practice
- Published
- 2024-11-26
- DOI
- https://doi.org/10.5005/jp-journals-10024-3744
- Citations
- 3
- Primary Topic
- Dental materials and restorations
- Type
- article
- Field-Weighted Citation Impact
- 1.21