Dense and uniform Mo10W alloy prepared by combining a vacuum sintering process with a hot-pressing process

Mo10W billets are fabricated via vacuum sintering (VS), hot pressing (HP), and VS + HP process. The results show that the Mo10W prepared by VS has good uniformity, even when the sintering temperature is as low as 1600 °C. However, the relative density of this alloy is only 95.37% when the sintering temperature is increased to 1900 °C. A high sintering temperature coarsens the grains. The relative density of HP-based Mo10W reaches 99.05% after sintering at 1500 °C, but its distributions of Mo and W are uneven. The Mo and W distributions of the VS + HP Mo10W alloy are uniform and its relative density reaches 98.1%. This work provides a new method for simultaneously improving the uniformity and density characteristics of Mo alloys.

Authors

Institutions

Publication Details

Journal
Materials Science and Technology
Published
2024-11-26
DOI
https://doi.org/10.1177/02670836241302687
Primary Topic
Advanced materials and composites
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Dense and uniform Mo10W alloy prepared by combining a vacuum sintering process with a hot-pressing process

Wenbo Cao, Xiaochao Wu, Chengduo Wang, Qingkui Li et al.
Materials Science and Technology
Advanced materials and composites
article

Dense and uniform Mo10W alloy prepared by combining a vacuum sintering process with a hot-pressing process

Wenbo Cao, Xiaochao Wu, Chengduo Wang, Qingkui Li, Hao Song, Pengzhan Ding
article en

Abstract

Mo10W billets are fabricated via vacuum sintering (VS), hot pressing (HP), and VS + HP process. The results show that the Mo10W prepared by VS has good uniformity, even when the sintering temperature is as low as 1600 °C. However, the relative density of this alloy is only 95.37% when the sintering temperature is increased to 1900 °C. A high sintering temperature coarsens the grains. The relative density of HP-based Mo10W reaches 99.05% after sintering at 1500 °C, but its distributions of Mo and W are uneven. The Mo and W distributions of the VS + HP Mo10W alloy are uniform and its relative density reaches 98.1%. This work provides a new method for simultaneously improving the uniformity and density characteristics of Mo alloys.

Materials Science and TechnologyVol. 42(4)
Zhengzhou University (CN)
National Natural Science Foundation of China
Affordable and clean energy
Openalex Percentile: Top 78%
Advanced materials and composites
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.