Effect of adding ionic liquid into polydimethylsiloxane on the output performance of triboelectric nanogenerator

Abstract Adding 1-butyl-3-methylimidazolium bis(trifluoromethyl sulfonyl)imide (BMIM-TFSI), an ionic liquid, to polydimethylsiloxane (PDMS) films significantly enhances the output of triboelectric nanogenerators (TENGs). In a TENG using contact and separation between the composite film and an aluminum (Al) plate, incorporating 0.1 vol% of BMIM-TFSI more than doubled the output voltage achieved compared to a pure PDMS film. To understand the cause of this improvement, composition analysis around the surface of the composite polymer film was conducted before and after tapping. We found that BMIM-TFSI molecules segregated around the surface after tapping. It is considered that the polarization of the BMIM-TFSI molecules enhances the output performance of TENGs by superimposing on the surface charges generated at the PDMS/Al interface.

Authors

Institutions

Publication Details

Journal
Japanese Journal of Applied Physics
Published
2024-11-25
DOI
https://doi.org/10.35848/1347-4065/ad971c
Primary Topic
Advanced Sensor and Energy Harvesting Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of adding ionic liquid into polydimethylsiloxane on the output performance of triboelectric nanogenerator

Yumeng Zheng, Takashi Ikuno, Kentaro Kinoshita, Qingyang Zhou
Japanese Journal of Applied Physics
Advanced Sensor and Energy Harvesting Materials
article

Effect of adding ionic liquid into polydimethylsiloxane on the output performance of triboelectric nanogenerator

Yumeng Zheng, Takashi Ikuno, Kentaro Kinoshita, Qingyang Zhou
article en

Abstract

Abstract Adding 1-butyl-3-methylimidazolium bis(trifluoromethyl sulfonyl)imide (BMIM-TFSI), an ionic liquid, to polydimethylsiloxane (PDMS) films significantly enhances the output of triboelectric nanogenerators (TENGs). In a TENG using contact and separation between the composite film and an aluminum (Al) plate, incorporating 0.1 vol% of BMIM-TFSI more than doubled the output voltage achieved compared to a pure PDMS film. To understand the cause of this improvement, composition analysis around the surface of the composite polymer film was conducted before and after tapping. We found that BMIM-TFSI molecules segregated around the surface after tapping. It is considered that the polarization of the BMIM-TFSI molecules enhances the output performance of TENGs by superimposing on the surface charges generated at the PDMS/Al interface.

Japanese Journal of Applied PhysicsVol. 63(12)
Tokyo University of Science (JP)
Moritani Scholarship Foundation, Japan Society for the Promotion of Science
Openalex Percentile: Top 80%
Advanced Sensor and Energy Harvesting Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.