Investigation of critical copper release rates for dose optimization of antifouling coatings
Antifouling coatings are applied to ship and boat hulls to prevent the unwanted attachment of marine organisms known as biofouling. Most antifouling coatings do so through toxic means by continuously releasing copper from the paint film to the surrounding water and are thus of environmental concern. Few studies have investigated the minimum dose of copper from an antifouling coating required to inhibit biofouling, commonly referred to as the critical release rate. This study presents a comprehensive investigation into the critical release rates of copper from commercial antifouling coatings in European coastal waters, with study sites in the Atlantic (Arcachon, France), Kattegat (Hundested, Denmark) and Skagerrak (Tjärnö, Sweden). Employing a combination of X-ray Fluorescence (XRF) analysis and visual inspection, this six-month field study has evaluated the efficacy of various antifouling coatings with differing copper contents. The findings of this study indicate that a release rate of 7 μg cm −2 d −1 was sufficient to inhibit macrofoulers at all three sites during static conditions. Results also indicate that the critical release rate is a parameter that coating manufacturers can optimize, as the performance of the coatings was not solely dependent on the copper release rates. The general critical release rate of 7 μg cm −2 d −1 could serve as a benchmark for dose optimization of coatings for both the yacht and ship sectors in the studied waters to reduce their environmental impact. It can also be used as support for decision-makers to phase out coatings with unnecessarily high copper release rates from the market. • Minimum necessary release of copper from antifouling coatings investigated • Six-month field study at three different European coastal locations • Dose (copper release rate) coupled to coating efficacy (macrofouling inhibition) • 7 μg/cm 2 /day inhibits attachment of macroscopic fouling in all studied waters • Findings can be used for dose optimization of copper-based antifouling coatings
Authors
- Maria Lagerström (ORCID: https://orcid.org/0000-0002-7526-5295)
- Florane Le Bihanic
- Jérôme Cachot (ORCID: https://orcid.org/0000-0002-1492-9684)
- Ann I. Larsson (ORCID: https://orcid.org/0000-0003-3268-2037)
- Markus Schackmann (ORCID: https://orcid.org/0009-0007-4303-4146)
- Marcel Butschle (ORCID: https://orcid.org/0000-0002-6505-5278)
- Kim Dam‐Johansen (ORCID: https://orcid.org/0000-0003-1658-6176)
Institutions
- Centre National de la Recherche Scientifique (FR)
- Esslingen University of Applied Sciences (DE)
- Université de Bordeaux (FR)
- Environnements et Paléoenvironnements Océaniques et Continentaux (FR)
- French National Agency for Water and Aquatic Environments (FR)
- Institut Polytechnique de Bordeaux (FR)
- Chalmers University of Technology (SE)
- University of Gothenburg (SE)
- Technical University of Denmark (DK)
Publication Details
- Journal
- Progress in Organic Coatings
- Published
- 2024-11-20
- DOI
- https://doi.org/10.1016/j.porgcoat.2024.108928
- Citations
- 7
- Primary Topic
- Marine Biology and Environmental Chemistry
- Type
- article
- Field-Weighted Citation Impact
- 2.35
Funders
- Svenska Forskningsrådet Formas
- Delhi Technological University
- Council on Ocean Affairs Science and Technology, California State University