Ionic Liquid Additive Mitigating Lithium Loss and Aluminum Corrosion for High-Voltage Anode-Free Lithium Metal Batteries

Concentrated electrolytes based on lithium bis(fluorosulfonyl)imide (LiFSI) have been proposed as an effective Li-compatible electrolyte for anode-free lithium metal batteries (AFLMBs). However, these electrolytes suffer from severe aluminum corrosion at an elevated potential. To address this issue, we propose a binary ionic liquid (IL) electrolyte additive comprising the 1-methyl-1-butyl pyrrolidinium cation (Pyr<sub>14</sub><sup>+</sup>), difluoro(oxalate)borate anion (DFOB<sup>-</sup>), and difluorophosphate (PO<sub>2</sub>F<sub>2</sub><sup>-</sup>) anion to mitigate the Li inventory loss and Al corrosion in 4 M LiFSI/DME electrolyte simultaneously. On the anode side, the IL additive facilitates the formation of a robust Li<sub>3</sub>N- and LiF-rich solid electrolyte interphase, promoting highly reversible Li plating/stripping and uniform Li deposition. Additionally, the ILs alter the Li<sup>+</sup> solvation structure, leading to enhanced <i>t</i><sub>Li<sup>+</sup></sub> and rapid Li<sup>+</sup> desolvation kinetics. Concurrently, on the cathode side, the ILs aid in the generation of dense LiF- and AlF-rich passivation films against Al corrosion. By using the IL-added electrolyte, the Cu||LiMn<sub>0.7</sub>Fe<sub>0.3</sub>PO<sub>4</sub> cell operates stably at 4.5 V, and the Cu||NCM613 cell with a high loading of 4.0 mA h cm<sup>-2</sup> sustains 142 cycles until 80% capacity retention. This research contributes to a deeper understanding of the IL additive mechanism at the electrode-electrolyte interfaces and offers a straightforward approach to designing practical high-voltage AFLMB electrolytes.

Authors

Institutions

Publication Details

Journal
ACS Nano
Published
2024-11-15
DOI
https://doi.org/10.1021/acsnano.4c13203
Citations
30
Primary Topic
Advanced Battery Materials and Technologies
Type
article
Field-Weighted Citation Impact
6.26

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Ionic Liquid Additive Mitigating Lithium Loss and Aluminum Corrosion for High-Voltage Anode-Free Lithium Metal Batteries

Qili Su, Minghan Zhou, Shiguo Zhang, Xueao Jiang et al.
30 citations
ACS Nano
Advanced Battery Materials and Technologies
6.26
article

Ionic Liquid Additive Mitigating Lithium Loss and Aluminum Corrosion for High-Voltage Anode-Free Lithium Metal Batteries

Qili Su, Minghan Zhou, Shiguo Zhang, Xueao Jiang, Zhe Li, Zhengjian Chen, Xiwen Wang, Weijian Liu, Haijing Liu, Xuansheng Wu, Junfeng Zeng
article en
30 citations

Abstract

Concentrated electrolytes based on lithium bis(fluorosulfonyl)imide (LiFSI) have been proposed as an effective Li-compatible electrolyte for anode-free lithium metal batteries (AFLMBs). However, these electrolytes suffer from severe aluminum corrosion at an elevated potential. To address this issue, we propose a binary ionic liquid (IL) electrolyte additive comprising the 1-methyl-1-butyl pyrrolidinium cation (Pyr<sub>14</sub><sup>+</sup>), difluoro(oxalate)borate anion (DFOB<sup>-</sup>), and difluorophosphate (PO<sub>2</sub>F<sub>2</sub><sup>-</sup>) anion to mitigate the Li inventory loss and Al corrosion in 4 M LiFSI/DME electrolyte simultaneously. On the anode side, the IL additive facilitates the formation of a robust Li<sub>3</sub>N- and LiF-rich solid electrolyte interphase, promoting highly reversible Li plating/stripping and uniform Li deposition. Additionally, the ILs alter the Li<sup>+</sup> solvation structure, leading to enhanced <i>t</i><sub>Li<sup>+</sup></sub> and rapid Li<sup>+</sup> desolvation kinetics. Concurrently, on the cathode side, the ILs aid in the generation of dense LiF- and AlF-rich passivation films against Al corrosion. By using the IL-added electrolyte, the Cu||LiMn<sub>0.7</sub>Fe<sub>0.3</sub>PO<sub>4</sub> cell operates stably at 4.5 V, and the Cu||NCM613 cell with a high loading of 4.0 mA h cm<sup>-2</sup> sustains 142 cycles until 80% capacity retention. This research contributes to a deeper understanding of the IL additive mechanism at the electrode-electrolyte interfaces and offers a straightforward approach to designing practical high-voltage AFLMB electrolytes.

ACS NanoVol. 18(47)
Hunan University (CN), Chinese Academy of Sciences (CN), SAIC-GM (China) (CN), Zhuhai Institute of Advanced Technology (CN)
National Natural Science Foundation of China, Natural Science Foundation of Hunan Province, State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Guangxi Key Laboratory of Electrochemical and Magnetochemical Functional Materials
Affordable and clean energy
Openalex Percentile: Top 3%
Advanced Battery Materials and Technologies
6.26
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.