Effect of liquid droplet impingement on electrochemical passivation behavior of 321 stainless steel in 0.5 wt% NaCl solution

Liquid droplet impingement (LDI) treatment changes the roughness and introduces residual compressive stress on 321 stainless steel (SS). Compared to untreated 321 SS, 1 h of LDI treatment with 100, 150 and 175 m/s gradually increases the pitting potential of 321 SS, while 1 h of LDI treatment with 200 m/s decreased the pitting potential of 321 SS. The passive films grown on the 321 SS after LDI treatment with 100, 150 and 175 m/s show a decreased receptor density, an increased Cr content and an increased thickness, whereas a dense passive film with good corrosion resistance cannot be formed on the 321 SS after LDI treatment with 200 m/s. The effect of the change in surface state due to LDI treatment on the electrochemical passivation behavior is explained in detail.

Authors

Institutions

Publication Details

Journal
Journal of Materials Research and Technology
Published
2024-11-01
DOI
https://doi.org/10.1016/j.jmrt.2024.11.138
Citations
3
Primary Topic
Hydrogen embrittlement and corrosion behaviors in metals
Type
article
Field-Weighted Citation Impact
0.52

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of liquid droplet impingement on electrochemical passivation behavior of 321 stainless steel in 0.5 wt% NaCl solution

Rui Liu, Yu Cui, Fuhui Wang, Li Liu et al.
3 citations
Journal of Materials Research and Technology
Hydrogen embrittlement and corrosion behaviors in metals
0.52
article

Effect of liquid droplet impingement on electrochemical passivation behavior of 321 stainless steel in 0.5 wt% NaCl solution

Rui Liu, Yu Cui, Fuhui Wang, Li Liu, Shuangyu Du, Weihai Xue
article en
3 citations

Abstract

Liquid droplet impingement (LDI) treatment changes the roughness and introduces residual compressive stress on 321 stainless steel (SS). Compared to untreated 321 SS, 1 h of LDI treatment with 100, 150 and 175 m/s gradually increases the pitting potential of 321 SS, while 1 h of LDI treatment with 200 m/s decreased the pitting potential of 321 SS. The passive films grown on the 321 SS after LDI treatment with 100, 150 and 175 m/s show a decreased receptor density, an increased Cr content and an increased thickness, whereas a dense passive film with good corrosion resistance cannot be formed on the 321 SS after LDI treatment with 200 m/s. The effect of the change in surface state due to LDI treatment on the electrochemical passivation behavior is explained in detail.

Journal of Materials Research and TechnologyVol. 33
International Centre for Materials Physics (CN), Northeastern University (CN)
National Natural Science Foundation of China
Openalex Percentile: Top 44%
Hydrogen embrittlement and corrosion behaviors in metals
0.52
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.