Measurement of ambient fiber and fibrous glass concentrations near three fiberglass wool manufacturing facilities in the United States

A limited number of published studies have evaluated concentrations of airborne fibers in outdoor air, with even fewer assessing typical air concentrations in the ambient air near fiberglass wool manufacturing facilities. Building upon the assessment by Switala et al. (1994), area samples for airborne fiber concentrations (diameters of less than 3 µm, lengths greater than 5 µm, and aspect ratios equal to or greater than 5 to 1) were collected at fixed locations along the fence lines of three fiberglass wool manufacturing facilities in the United States. Samples were analyzed by the National Institute for Occupational Safety and Health (NIOSH) Method 7400, via phase contrast microscopy (PCM) using "B" counting rules. A total of 134 samples were collected across the three plants. Overall, 73% of the samples collected were below the limit of quantification (LOQ). Using the Kaplan-Meier (KM) method for estimation of values below the LOQ, the geometric mean fiber concentration for all plants combined was 0.0028 fibers per cubic centimeter (f/cc), with the 95<sup>th</sup> percentile upper confidence level at 0.0049 f/cc. Of those samples with detectable concentrations of airborne fibers (<i>n</i> = 36), when further analyzed using energy dispersive X-ray (EDX) analysis, only one sample had a detectable glass fiber concentration at 0.0045 f/cc, which was noted as the detection limit for the method. This glass fiber concentration is within the range anticipated for ambient fibrous glass near production facilities, suggesting consistency with measurements made by Switala et al. (1994), despite changes in production methods (i.e., use of different binders) since 1994 and the use of updated methods for treatment of values below the LOQ in the current assessment.

Authors

Institutions

Publication Details

Journal
Journal of Occupational and Environmental Hygiene
Published
2024-11-11
DOI
https://doi.org/10.1080/15459624.2024.2406229
Citations
1
Primary Topic
Textile materials and evaluations
Type
article
Field-Weighted Citation Impact
0.17
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Measurement of ambient fiber and fibrous glass concentrations near three fiberglass wool manufacturing facilities in the United States

Andrew Maier, Laura H. Allen, H. V. Fairbanks, Chloe Stewart et al.
1 citations
Journal of Occupational and Environmental Hygiene
Textile materials and evaluations
0.17
article

Measurement of ambient fiber and fibrous glass concentrations near three fiberglass wool manufacturing facilities in the United States

Andrew Maier, Laura H. Allen, H. V. Fairbanks, Chloe Stewart, Natalie Suder Egnot, P.J. Wells
article en
1 citations

Abstract

A limited number of published studies have evaluated concentrations of airborne fibers in outdoor air, with even fewer assessing typical air concentrations in the ambient air near fiberglass wool manufacturing facilities. Building upon the assessment by Switala et al. (1994), area samples for airborne fiber concentrations (diameters of less than 3 µm, lengths greater than 5 µm, and aspect ratios equal to or greater than 5 to 1) were collected at fixed locations along the fence lines of three fiberglass wool manufacturing facilities in the United States. Samples were analyzed by the National Institute for Occupational Safety and Health (NIOSH) Method 7400, via phase contrast microscopy (PCM) using "B" counting rules. A total of 134 samples were collected across the three plants. Overall, 73% of the samples collected were below the limit of quantification (LOQ). Using the Kaplan-Meier (KM) method for estimation of values below the LOQ, the geometric mean fiber concentration for all plants combined was 0.0028 fibers per cubic centimeter (f/cc), with the 95<sup>th</sup> percentile upper confidence level at 0.0049 f/cc. Of those samples with detectable concentrations of airborne fibers (<i>n</i> = 36), when further analyzed using energy dispersive X-ray (EDX) analysis, only one sample had a detectable glass fiber concentration at 0.0045 f/cc, which was noted as the detection limit for the method. This glass fiber concentration is within the range anticipated for ambient fibrous glass near production facilities, suggesting consistency with measurements made by Switala et al. (1994), despite changes in production methods (i.e., use of different binders) since 1994 and the use of updated methods for treatment of values below the LOQ in the current assessment.

Journal of Occupational and Environmental HygieneVol. 22(1)
Stantec (United States) (US), Stantec (Canada) (CA)
Openalex Percentile: Top 57%
Textile materials and evaluations
0.17
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.