DETERMINATION OF TECHNOLOGICAL CHARACTERISTICS OF PRESSABILITY
This article deals with the results of technological tests of pressability (Erichsen's - IE index and capping - limit drawing ratio (LDR)). It also presents on which material parameter (ductility, strain hardening exponent, coefficient of normal anisotropy...) should be given more emphasis when choosing a steel sheet, if stretching stress (uniaxial tension, biaxial tension) dominates during the production of stampings, or if dominates the “pull-pressure” technique (pulling out from under the flange).
Authors
- JAROSLAV SOLTES
- Jozef Pavelka
- JOZEF KMEC
Publication Details
- Journal
- MM Science Journal
- Published
- 2024-11-05
- DOI
- https://doi.org/10.17973/mmsj.2024_11_2024021
- Primary Topic
- Engineering Diagnostics and Reliability
- Type
- article
- Field-Weighted Citation Impact
- 0.00