The Anti/Deicing Performance of the Low Interfacial Toughness Coating Is Enhanced: Induced Ice Crack Generation and Its Extension

The low interfacial toughness of the material surface is important for crack initiation and expansion of the ice layer as it remains an effective method for large-scale deicing. However, there are challenges, such as a large critical icing size and incomplete shedding of the ice layer. Adjusting the interfacial forces to make the ice more prone to cracking, expanding, and shedding is advantageous in addressing the problem of anti-icing failure in materials with low interfacial toughness. Therefore, we propose a deicing strategy that combines porous PDMS (polydimethylsiloxane) coatings with low interfacial toughness and piezoelectric vibration. A series of hydrophobic porous PDMS coatings with different porosities were prepared on the surface of an aluminum alloy substrate through curing and phase separation. The elastic modulus of the coatings decreased from 1465 to 509 kPa as the coating porosity increased, revealing the mechanism behind the improvement in mechanical properties. The key to promoting ice fracture on porous PDMS coatings lies in the synergistic effect of the out-of-plane shear stress and microcracks at the solid-ice interface. This work focuses on exploring the characteristics of interfacial forces by combining the intrinsic mechanical properties of coatings with external forces, providing new insights for designing low interfacial toughness anti-icing materials.

Authors

Institutions

Publication Details

Journal
Langmuir
Published
2024-11-05
DOI
https://doi.org/10.1021/acs.langmuir.4c03672
Citations
6
Primary Topic
Icing and De-icing Technologies
Type
article
Field-Weighted Citation Impact
7.79

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

The Anti/Deicing Performance of the Low Interfacial Toughness Coating Is Enhanced: Induced Ice Crack Generation and Its Extension

Senyun Liu, Yizhou Shen, Weilan Liu, Lingfeng Zhao et al.
6 citations
Langmuir
Icing and De-icing Technologies
7.79
article

The Anti/Deicing Performance of the Low Interfacial Toughness Coating Is Enhanced: Induced Ice Crack Generation and Its Extension

Senyun Liu, Yizhou Shen, Weilan Liu, Lingfeng Zhao, Bingquan Wu, Junjian He
article en
6 citations

Abstract

The low interfacial toughness of the material surface is important for crack initiation and expansion of the ice layer as it remains an effective method for large-scale deicing. However, there are challenges, such as a large critical icing size and incomplete shedding of the ice layer. Adjusting the interfacial forces to make the ice more prone to cracking, expanding, and shedding is advantageous in addressing the problem of anti-icing failure in materials with low interfacial toughness. Therefore, we propose a deicing strategy that combines porous PDMS (polydimethylsiloxane) coatings with low interfacial toughness and piezoelectric vibration. A series of hydrophobic porous PDMS coatings with different porosities were prepared on the surface of an aluminum alloy substrate through curing and phase separation. The elastic modulus of the coatings decreased from 1465 to 509 kPa as the coating porosity increased, revealing the mechanism behind the improvement in mechanical properties. The key to promoting ice fracture on porous PDMS coatings lies in the synergistic effect of the out-of-plane shear stress and microcracks at the solid-ice interface. This work focuses on exploring the characteristics of interfacial forces by combining the intrinsic mechanical properties of coatings with external forces, providing new insights for designing low interfacial toughness anti-icing materials.

LangmuirVol. 40(46)
Nanjing Tech University (CN), China Aerodynamics Research and Development Center (CN), State Key Laboratory of Aerodynamics, Nanjing University of Aeronautics and Astronautics (CN)
National Natural Science Foundation of China, Natural Science Foundation of Jiangsu Province, Chinese Aeronautical Establishment, Priority Academic Program Development of Jiangsu Higher Education Institutions, National Science and Technology Major Project, Fundamental Research Funds for the Central Universities
Openalex Percentile: Top 3%
Icing and De-icing Technologies
7.79
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.