Mechanical Response of Hot-Mixed Epoxy Asphalt Concrete Steel Deck Pavement Under Thermal and Load

In recent years, fatigue cracking in orthotropic steel bridge deck pavements has become a significant concern, so the investigation of the mechanical response of the pavement layer has become a central focus in pavement structure design. This experiment subjected a full-scale specimen to a constant amplitude dynamic load of 60 kN to 300 kN over 2 million cycles. Throughout the testing, a circulating water bath elevated the temperature of the pavement layer from 15 °C to 50 °C. Key locations were monitored for strain and deflection data, facilitating an investigation into the mechanical response of the epoxy asphalt pavement system under the effects of temperature and load. The results indicate that the maximum transverse strain at the bottom of the steel deck occurs at the U-rib weld aligned with the load center, reaching 190% of the initial loading strain. Meanwhile, the maximum transverse strain on the pavement surface is observed at the U-rib weld adjacent to the loaded area, measuring 167% of the initial strain. The maximum longitudinal strain is lower than the maximum transverse strain. In the load zone, the longitudinal strain between the U-ribs exceeds that at the U-rib weld. Both transverse strain and relative deflection increase as the load intensifies. The relationship between transverse strain and applied load is characterized by an exponential function, while deflection exhibits a cubic relationship with the applied load. Elevated temperatures also contribute to increased transverse strains at both the bottom of the steel deck and the pavement surface, following an exponential trend. Relative deflection is primarily influenced by the applied load and remains relatively unaffected by temperature variations. When accounting for the coupling of load and temperature, the maximum transverse strains at both the bottom of the steel deck and the pavement surface can be modeled as an exponential function of the independent variables: load and temperature.

Authors

Institutions

Publication Details

Journal
Buildings
Published
2024-10-31
DOI
https://doi.org/10.3390/buildings14113482
Primary Topic
Asphalt Pavement Performance Evaluation
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Mechanical Response of Hot-Mixed Epoxy Asphalt Concrete Steel Deck Pavement Under Thermal and Load

Peiwei Gao, Min Li, Lei Cui, Xuan Xu et al.
Buildings
Asphalt Pavement Performance Evaluation
article

Mechanical Response of Hot-Mixed Epoxy Asphalt Concrete Steel Deck Pavement Under Thermal and Load

Peiwei Gao, Min Li, Lei Cui, Xuan Xu, Hui Zhang, Guoqing Li, R.C. Luo
article en

Abstract

In recent years, fatigue cracking in orthotropic steel bridge deck pavements has become a significant concern, so the investigation of the mechanical response of the pavement layer has become a central focus in pavement structure design. This experiment subjected a full-scale specimen to a constant amplitude dynamic load of 60 kN to 300 kN over 2 million cycles. Throughout the testing, a circulating water bath elevated the temperature of the pavement layer from 15 °C to 50 °C. Key locations were monitored for strain and deflection data, facilitating an investigation into the mechanical response of the epoxy asphalt pavement system under the effects of temperature and load. The results indicate that the maximum transverse strain at the bottom of the steel deck occurs at the U-rib weld aligned with the load center, reaching 190% of the initial loading strain. Meanwhile, the maximum transverse strain on the pavement surface is observed at the U-rib weld adjacent to the loaded area, measuring 167% of the initial strain. The maximum longitudinal strain is lower than the maximum transverse strain. In the load zone, the longitudinal strain between the U-ribs exceeds that at the U-rib weld. Both transverse strain and relative deflection increase as the load intensifies. The relationship between transverse strain and applied load is characterized by an exponential function, while deflection exhibits a cubic relationship with the applied load. Elevated temperatures also contribute to increased transverse strains at both the bottom of the steel deck and the pavement surface, following an exponential trend. Relative deflection is primarily influenced by the applied load and remains relatively unaffected by temperature variations. When accounting for the coupling of load and temperature, the maximum transverse strains at both the bottom of the steel deck and the pavement surface can be modeled as an exponential function of the independent variables: load and temperature.

BuildingsVol. 14(11)
Nanjing University of Aeronautics and Astronautics (CN)
National Key Research and Development Program of China
Sustainable cities and communities
Openalex Percentile: Top 78%
Asphalt Pavement Performance Evaluation
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.