Recovery of Xenotime and Florencite from Silicate Minerals Using a Combined Technique of Magnetic Separation and Flotation
Xenotime (YPO4), a significant phosphatic minerl rich in heavy rare earth elements (HREEs), typically associates with granitic rocks, exemplified in the Wolverine rare earth deposit in Australia. A mineral composition analysis indicates that the primary valuable minerals in the deposit are principally xenotime and minor florencite, with quartz and illite as the main gangue minerals, showing a relatively simple mineral composition. The grade of rare earth concentrate was increased to 14.29% and the recovery reached 94.48% through the magnetic separation pre-enrichment test. However, a high-grade rare earth concentrate could not be achieved using magnetic separation alone. Further purification of the magnetic concentrate is conducted through flotation. The grade of rare earth concentrate reached 51.26%, and the recovery rate reached 90.47%. In summary, this process achieves the efficient recovery of xenotime and florencite, having substantial industrial potential.
Authors
- Weiyao Zhu (ORCID: https://orcid.org/0000-0003-0074-4934)
- Erdou Li
- Weiwei Wang (ORCID: https://orcid.org/0000-0002-6640-7503)
- Zhengyao Li (ORCID: https://orcid.org/0000-0001-9259-0017)
- Yuanyuan Wang (ORCID: https://orcid.org/0000-0002-5576-6375)
Institutions
- Baotou Research Institute of Rare Earths (CN)
- University of Science and Technology Beijing (CN)
Publication Details
- Journal
- Minerals
- Published
- 2024-10-25
- DOI
- https://doi.org/10.3390/min14111073
- Citations
- 3
- Primary Topic
- Metal Extraction and Bioleaching
- Type
- article
- Field-Weighted Citation Impact
- 0.55
Funders
- Natural Science Foundation of Inner Mongolia