Ca(Mo,W)O<sub>4</sub> Solid Solutions Formation in CaMoO<sub>4</sub>‐CaWO<sub>4</sub> System

Abstract The formation of solid solutions in the CaMoO 4 ‐CaWO 4 binary system is investigated by X‐ray diffraction, Raman spectroscopy, and scanning electron microscopy methods. The intermixtures of CaMoO 4 and CaWO 4 components are sintered in 600—1200 °C temperature range (in 100 °C increments). The solidus of the CaMo x W (1‐x) O 4 system is studied by the differential scanning calorimetry method in the x = 0.3 … 1.0 range. CaMoO 4 ‐CaWO 4 phase diagram is constructed up to 1550 °C. The minimal sintering temperature in order to get CaMo x W (1‐x) O 4 solid solution is shown to be 800 °C. Cathodoluminescence study of CaMo x W (1‐x) O 4 compounds showed higher intensity of molybdate luminescence type.

Authors

Institutions

Publication Details

Journal
Crystal Research and Technology
Published
2024-10-25
DOI
https://doi.org/10.1002/crat.202400127
Primary Topic
Luminescence Properties of Advanced Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Ca(Mo,W)O4 Solid Solutions Formation in CaMoO4‐CaWO4 System

A.E. Musikhin, K.A. Kokh, Alexey A. Ryadun, A.B. Kuznetsov et al.
Crystal Research and Technology
Luminescence Properties of Advanced Materials
article

Ca(Mo,W)O4 Solid Solutions Formation in CaMoO4‐CaWO4 System

A.E. Musikhin, K.A. Kokh, Alexey A. Ryadun, A.B. Kuznetsov, V. D. Grigorieva, D.M. Khramtsova
article en

Abstract

Abstract The formation of solid solutions in the CaMoO 4 ‐CaWO 4 binary system is investigated by X‐ray diffraction, Raman spectroscopy, and scanning electron microscopy methods. The intermixtures of CaMoO 4 and CaWO 4 components are sintered in 600—1200 °C temperature range (in 100 °C increments). The solidus of the CaMo x W (1‐x) O 4 system is studied by the differential scanning calorimetry method in the x = 0.3 … 1.0 range. CaMoO 4 ‐CaWO 4 phase diagram is constructed up to 1550 °C. The minimal sintering temperature in order to get CaMo x W (1‐x) O 4 solid solution is shown to be 800 °C. Cathodoluminescence study of CaMo x W (1‐x) O 4 compounds showed higher intensity of molybdate luminescence type.

Crystal Research and TechnologyVol. 59(11)
Novosibirsk State University (RU), V.S. Sobolev Institute of Geology and Mineralogy (RU), Siberian Branch of the Russian Academy of Sciences (RU), Nikolaev Institute of Inorganic Chemistry (RU)
Russian Science Foundation
Openalex Percentile: Top 88%
Luminescence Properties of Advanced Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.