Effect of Ti–Mg–Ce Complex Deoxidation on the Inclusions and Mechanical Properties of S355 Steel

Oxide metallurgy technology not only refines the microstructure but also modifies the type, density, and size of inclusions. This study examines the impact of Ti–Mg–Ce composite deoxidation on the inclusions and mechanical properties of S355 steel used for heavy‐duty H‐beams. Compared to base alloy, Ti–Mg–Ce‐added alloy features a higher presence of inclusions such as MgO, TiN (containing Ce), TiO x , and TiS, except for SiO 2 , Al 2 O 3 , MnS, and MnO. Following Ti–Mg–Ce composite deoxidation, the number density of inclusions increases by 16.4%, and the equivalent diameter, length, and width of the inclusions decrease by 41.0%, 41.2%, and 37.9%, respectively. The length of large‐angle grain boundaries in the same area increases by 20%, and the average grain size reduces by 12.5%, resulting in an enhancement of yield strength by 23.6 MPa, tensile strength by 37 MPa, total elongation by 2.1%, and impact energy by 92 J. By employing Ti–Mg–Ce composite deoxidation to optimize inclusions and microstructure, the strength, plasticity, and toughness of the experimental steel are significantly improved.

Authors

Institutions

Publication Details

Journal
steel research international
Published
2024-10-22
DOI
https://doi.org/10.1002/srin.202400658
Primary Topic
Metallurgical Processes and Thermodynamics
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Effect of Ti–Mg–Ce Complex Deoxidation on the Inclusions and Mechanical Properties of S355 Steel

Tianrui Li, Liangliang Zhang, Zhiqiang Chen, Xiangjun Zhang et al.
steel research international
Metallurgical Processes and Thermodynamics
article

Effect of Ti–Mg–Ce Complex Deoxidation on the Inclusions and Mechanical Properties of S355 Steel

Tianrui Li, Liangliang Zhang, Zhiqiang Chen, Xiangjun Zhang, Yong Yang, Yong Xu, Wen‐Ping Wu, Yong Lv
article en

Abstract

Oxide metallurgy technology not only refines the microstructure but also modifies the type, density, and size of inclusions. This study examines the impact of Ti–Mg–Ce composite deoxidation on the inclusions and mechanical properties of S355 steel used for heavy‐duty H‐beams. Compared to base alloy, Ti–Mg–Ce‐added alloy features a higher presence of inclusions such as MgO, TiN (containing Ce), TiO x , and TiS, except for SiO 2 , Al 2 O 3 , MnS, and MnO. Following Ti–Mg–Ce composite deoxidation, the number density of inclusions increases by 16.4%, and the equivalent diameter, length, and width of the inclusions decrease by 41.0%, 41.2%, and 37.9%, respectively. The length of large‐angle grain boundaries in the same area increases by 20%, and the average grain size reduces by 12.5%, resulting in an enhancement of yield strength by 23.6 MPa, tensile strength by 37 MPa, total elongation by 2.1%, and impact energy by 92 J. By employing Ti–Mg–Ce composite deoxidation to optimize inclusions and microstructure, the strength, plasticity, and toughness of the experimental steel are significantly improved.

steel research internationalVol. 96(3)
MCC Huatian Engineering and Technology Corporation (CN), Shougang Institute of Technology (CN), Anhui University of Technology (CN)
National Natural Science Foundation of China, Scientific Research and Technology Development Program of Guangxi
Openalex Percentile: Top 82%
Metallurgical Processes and Thermodynamics
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.