A strategy for introducing biopotency-enhanced chirality coating on bio-magnesium

• The chiral supramolecular hydrogel was used to simulate the chiral environment of biological systems and enhance the adsorption of osteogenic growth factors. • Theoretical calculations confirmed that the chirality enhancement was attributed to the spatial structure recognition of the left-handed fibers to the right-handed α-helical segments. • The silane layers pretreated on Mg surface enhanced the corrosion resistance while introducing active functional groups conducive to the binding of supramolecular fibers. Biomedical magnesium alloys (Mg) are often considered potential metallic materials for bone repair scaffolds due to their excellent biomechanical properties, biocompatibility, and biodegradability. However, their rapid degradation behavior is insufficient to support the rapid growth and repair of living tissues. The new surface modification methods to slow down the degradation rate of Mg scaffolds and promote the rapid growth of living tissues is urgent. Here, we developed a chiral-enhanced composite functional coating on the surface of biomedical magnesium. Specifically, a chiral supramolecular hydrogel with graphene oxide (GO) was used to simulate the chiral environment of biological systems, enhancing the adsorption of osteogenic growth factors. Additionally, the silane layers cleverly crosslink traditional silane chains with supramolecular chiral fibers through a hydrogen bond network, which allows the bonding strength (critical loads) of the composite coating to be maintained between 245–275 mN and retains structural integrity when soaked in SBF for 7 days. It was found that both MC3T3-E1 cells growth and BMP-2 adhesion were significantly enhanced by GO-added left-handed chiral coatings, which exhibit superior bone growth-promoting effects. In summary, incorporating chiral features into functional coatings represents a transformative approach in the design and application of bone defect repair materials.

Authors

Institutions

Publication Details

Journal
Materials & Design
Published
2024-10-20
DOI
https://doi.org/10.1016/j.matdes.2024.113372
Citations
2
Primary Topic
Bone Tissue Engineering Materials
Type
article
Field-Weighted Citation Impact
0.37

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

A strategy for introducing biopotency-enhanced chirality coating on bio-magnesium

Wenjiang Huang, Chuanliang Feng, Shaokang Guan, Xiaxin Qiu et al.
2 citations
Materials & Design
Bone Tissue Engineering Materials
0.37
article

A strategy for introducing biopotency-enhanced chirality coating on bio-magnesium

Wenjiang Huang, Chuanliang Feng, Shaokang Guan, Xiaxin Qiu, Jinying Liu, Qichao Zhao, Yu Zhao, Delin Ma
article en
2 citations

Abstract

• The chiral supramolecular hydrogel was used to simulate the chiral environment of biological systems and enhance the adsorption of osteogenic growth factors. • Theoretical calculations confirmed that the chirality enhancement was attributed to the spatial structure recognition of the left-handed fibers to the right-handed α-helical segments. • The silane layers pretreated on Mg surface enhanced the corrosion resistance while introducing active functional groups conducive to the binding of supramolecular fibers. Biomedical magnesium alloys (Mg) are often considered potential metallic materials for bone repair scaffolds due to their excellent biomechanical properties, biocompatibility, and biodegradability. However, their rapid degradation behavior is insufficient to support the rapid growth and repair of living tissues. The new surface modification methods to slow down the degradation rate of Mg scaffolds and promote the rapid growth of living tissues is urgent. Here, we developed a chiral-enhanced composite functional coating on the surface of biomedical magnesium. Specifically, a chiral supramolecular hydrogel with graphene oxide (GO) was used to simulate the chiral environment of biological systems, enhancing the adsorption of osteogenic growth factors. Additionally, the silane layers cleverly crosslink traditional silane chains with supramolecular chiral fibers through a hydrogen bond network, which allows the bonding strength (critical loads) of the composite coating to be maintained between 245–275 mN and retains structural integrity when soaked in SBF for 7 days. It was found that both MC3T3-E1 cells growth and BMP-2 adhesion were significantly enhanced by GO-added left-handed chiral coatings, which exhibit superior bone growth-promoting effects. In summary, incorporating chiral features into functional coatings represents a transformative approach in the design and application of bone defect repair materials.

Materials & DesignVol. 247
Henan University (CN), Shanghai Jiao Tong University (CN), Zhengzhou University (CN), Xuchang University (CN)
National Natural Science Foundation of China
Openalex Percentile: Top 43%
Bone Tissue Engineering Materials
0.37
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.